Welding method of steel reinforcement strip welding

A welding method and technology for bar welding, applied in welding equipment, arc welding equipment, manufacturing tools, etc., can solve the problems of low production efficiency, unstable welding quality, affecting welding quality, etc., so as to improve production efficiency and increase welding speed. Effect

Active Publication Date: 2013-02-27
STATE GRID CORP OF CHINA +1
View PDF7 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Welding of steel bar by using electrode arc welding welding method, due to the characteristics of this welding method, it has the disadvantages of low production efficiency and unstable welding quality
And solid wire CO 2 Semi-automatic gas shielded welding itself is a low-hydrogen welding method. Before welding, the steel surface is required to be clean and free of dirt, but there are rust and other dirt on the surface of the steel bar during on-site welding. quality

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0017] To sum up, the present invention discloses a method for welding steel bars, comprising the following steps:

[0018] The first step: the steel bars are paired, the ends of the steel bars to be welded are in contact with each other, and the side bars are placed on both sides of the steel bars to be welded;

[0019] The second step: positioning welding, pre-welding four positioning welding sections between the two steel bars to be welded and the two side bars, and connecting the steel bars to be welded and the side bars;

[0020] The third step: fixed welding, two steel bars and side bars to be welded are welded on both sides by flux-cored carbon dioxide gas shielded welding.

[0021] The four tack welding sections formed in the second tack welding process are located on the same side, and the length of the tack welding sections is 10-20mm.

[0022] The fixed welding step firstly welds the side without tack welding section, and secondly welds the side with ta...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
lengthaaaaaaaaaa
diameteraaaaaaaaaa
Login to View More

Abstract

The invention discloses a welding method of steel reinforcement strip welding. The welding method is characterized by comprising the following steps: 1, fitting up steel reinforcements, namely relatively contacting the end parts of the steel reinforcements to be welded, and placing strips on the two sides of each of the steel reinforcements to be welded; 2, carrying out positioned welding, namely pre-welding four positioned welding sections between the two steel reinforcements to be welded and the two strips, and connecting the steel reinforcements to be welded with the strips; and 3, carrying out fixed welding, namely welding the two steel reinforcements to be welded and the strips on the double surfaces by adopting flux-cored carbon dioxide arc welding. The method has the advantages as follows: a higher arc voltage is selected by utilizing a welding current and arc voltage ratio formula to guarantee sufficient heat for melting of welding wires and the steel reinforcements; the capabilities of a welding seam in resistance to dirt such as rust and resistance to a pore defect are improved by utilizing titanium calcium type slag formed after melting of powder in a flux-cored wire; and the welding speed is accelerated while necessary heat is guaranteed to enable the titanium calcium type slag in the welding wire to fully take part in metallurgical reaction, namely the production efficiency is improved by 2-3 times.

Description

technical field [0001] The invention relates to a welding method, in particular to a welding method for reinforcing bars. Background technique [0002] At present, in the existing steel bar welding in our country, the welding method of electrode arc welding is mainly used for connection. In recent years, a small amount of solid core welding wire CO has also appeared. 2 Semi-automatic gas shielded welding welding method. The use of arc welding welding method for steel bar welding has the disadvantages of low production efficiency and unstable welding quality due to the characteristics of the welding method itself. And solid wire CO 2 Semi-automatic gas shielded welding itself is a low-hydrogen welding method. Before welding, the steel surface is required to be clean and free of dirt, but there are rust and other dirt on the surface of the steel bar during on-site welding. quality. Contents of the invention [0003] The technical problem to be solved by the present inven...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B23K9/16
Inventor 王迎军张大刚何生贵焦荣格苏召王秉洪
Owner STATE GRID CORP OF CHINA
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products