Embodiment 1
[0034] The selected shirt cloth of this embodiment is: white 120*7680 / 2*80 / 2, 55% cotton / 45% real silk blended plain weave fabric.
[0035] The amount of resin Fixapret F-ECO (2D resin produced by BASF, Germany) in the aqueous solution of the finishing agent composition is 50g / L; the amount of water-soluble polyurethane finishing agent Perapret PU is 150g / L; the amount of strong protective agent Siligen PEP is 40g / L; softening agent Megasoft LUX dosage 50g / L; catalyst MgCl 2 The dosage is 10g / L, and the aqueous solution of the finishing agent composition is applied on the whole shirt through a spray machine, so that the liquid retention rate is 60%, and the liquid retention rate after pre-drying is controlled at about 20%. Use a portrait machine to blow and iron at 60°C for 30 seconds, and use a pressing machine at 170°C with a pressure of 0.5kg / cm 2 Press for 10 seconds, adjust the oven temperature to 160°C, and bake for 5 minutes. With the softening agent Cepreton UA p (...
Embodiment 2
[0039] The type of shirt fabric selected in this embodiment is: blue and white stripes 130×8680 / 2×80 / 2, interwoven 3 / 1 twill weave of cotton in the warp direction and silk in the weft direction. .
[0040] The amount of butane tetracarboxylic acid (BTCA) in the aqueous solution of the finishing agent composition is 60g / L; the amount of water-soluble polyurethane finishing agent Perapret PU is 200g / L; the amount of strong protective agent Siligen F-PEW is 30g / L; the amount of softener Siligen SIE is 20g / L; the amount of catalyst sodium hypophosphite is 20g / L, and the aqueous solution of the finishing agent composition is applied on the whole shirt through a spraying machine, so that the liquid accumulation rate is 90%, and the liquid accumulation rate is controlled at about 40% after pre-baking . Use a portrait machine to blow and iron at 100°C for 10 seconds, and use a pressing machine at 150°C to press 0.5kg / cm 2 Press for 7 seconds, adjust the oven temperature to 170°C, a...
PUM
Property | Measurement | Unit |
---|---|---|
concentration | aaaaa | aaaaa |
concentration | aaaaa | aaaaa |
concentration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com