Method for selecting copper sulphide ores in flotation manner
A technology for copper sulfide ore and dry ore, applied in flotation, solid separation and other directions, can solve the problems of high price, environmental hazards, poor selectivity, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] An ore containing mainly useful metal minerals such as chalcopyrite and pyrite, and gangue minerals such as quartz, containing 0.61% copper. Adjust the pH value of the pulp (lime can be added to the ball mill when using lime) to 8.5, and the concentration of the pulp is 35%, then add the collector 28g / t of ethyl thioglycolate dry ore to the pulp, stir for 2 minutes, and after a rough separation, you can get Copper sulfide rough concentrate.
[0018] The comparative test indicators of copper sulfide ore are shown in Table 1.
[0019] Table 1 Contrast of mineral processing index between using medicament in the present invention and using Z-200
[0020]
Embodiment 2
[0022] A kind of ore containing mainly useful metal minerals such as chalcopyrite and pyrite, and gangue minerals such as quartz, containing 0.57% copper. Adjust the pH value of the pulp (lime can be added to the ball mill when lime is used) to 7.5, and the concentration of the pulp is 35%, then add the collector agent ethyl thioglycolate 28g / t dry ore to the pulp, stir for 2 minutes, and after a rough separation, you can get Copper sulfide rough concentrate.
[0023] See Table 2 for the comparative test indicators of copper sulfide ore.
[0024] Table 2 Contrast of mineral processing index between using medicament in the present invention and using Z-200
[0025]
Embodiment 3
[0027] A kind of ore containing mainly useful metal minerals such as chalcopyrite and pyrite, and gangue minerals such as quartz, containing 0.59% copper. Adjust the pH value of the pulp (lime can be added to the ball mill when using lime) to 9.5, the concentration of the pulp is 35%, and then add the collector agent ethyl thioglycolate 15g / t dry ore to the pulp, stir for 2 minutes, and after a rough separation, you can get Copper sulfide rough concentrate.
[0028] See Table 3 for the comparative test indicators of copper sulfide ore.
[0029] Table 3 Contrast of mineral processing index between using medicament in the present invention and using Z-200
[0030]
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com