An environmentally responsive, nanoparticle technology, which is applied in non-active ingredient medical preparations, active ingredients-containing medical preparations, pharmaceutical formulas, etc., can solve problems such as strong cytotoxicity, and achieve good biocompatibility and good biocompatibility. Prospects of application, mild effect of reaction conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] pH-responsive nanoparticle drug delivery system with regulated release of sphingosine phosphate
[0032] (1) Template extraction method to prepare mesoporous silicon nanoparticles, the template agent hexadecyltrimethylammonium bromide was dissolved in sodium hydroxide solution at 50 °C, and ethyl orthosilicate was added dropwise, and vigorously stirred to produce The white precipitate was dried by suction filtration, refluxed with ethanol for 8 hours to remove the template, dried in vacuum, and stored for later use;
[0033] (2) Disperse the mesoporous silicon prepared in step 1 in toluene, add 3-aminopropyltriethoxysilane, the molar ratio of silicon dioxide, 3-aminopropyltriethoxysilane and toluene is 5: 1:500, reacted under nitrogen protection for 20 h, dried to obtain amino-modified mesoporous silicon nanoparticles, and preserved for future use;
[0034] (3) Make the amino-modified mesoporous silicon prepared in step 2 into a suspension (1.0-2.0wt.%), add sodium alg...
Embodiment 2
[0037] Preparation of pH-responsive nanoparticles loaded with doxorubicin
[0038] (1) Template extraction method to prepare mesoporous silicon nanoparticles, the template agent hexadecyltrimethylammonium bromide was dissolved in sodium hydroxide solution at 95 ° C, and tetraethyl orthosilicate was added dropwise, and vigorously stirred to produce The white precipitate was dried by suction filtration, refluxed with ethanol for 24 hours to remove the template, dried in vacuum, and stored for future use;
[0039](2) Make a suspension (1.0-2.0wt.%) of the mesoporous silicon nanoparticles prepared in step 1, add polyallylamine hydrochloride (1-2mg / mL), stir at room temperature for 0.2-2h, 4000r / min Centrifuge for 3min, wash, disperse to make a suspension, add sodium polystyrene sulfonate solution (1-2mg / mL), stir at room temperature for 0.2-2h, centrifuge at 4000r / min for 3min, wash, disperse to make a suspension, repeat the whole process 4 times, carry out self-installation laye...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
pore size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com