An ultrasonic couplant, disinfection and sterilization technology, applied in the field of couplant, can solve the problems of no chloramphenicol and polyhexamethylene guanidine, no skin detection, no disinfection and sterilization effect, etc., and achieves good sound conduction performance and fast speed. And long-term sterilization and disinfection function, bright color effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0045] 1. Feeding: according to the proportion of the formula, feed the material with a total amount of 1000g coupling agent, namely:
[0046]
[0047]
[0048] 2. Preparation method:
[0049] 1) Weighing various ingredients according to the prescription quantity;
[0050] 2) Add 5.0g of carbomer into 400g of deionized water, and stir in a water bath at 50-68°C until completely dissolved, and leave it;
[0051] 3) 1.0 g of 20% polyhexamethylene biguanide is completely dissolved in 30.0 g of glycerol, and left in place;
[0052] 4) Dissolve 3.0 g of chloramphenicol completely in 30 g of propylene glycol, and leave it;
[0053] 5) The 1.5g sodium hydroxide taken by weighing is completely dissolved in deionized water, and left
[0054] 6) Mix the mixed solution obtained in step 3) and 4) evenly, then add to the carbomer solution obtained in step 2) and stir until uniform, then add the remaining deionized water, and slowly add sodium hydroxide solution under stirring Sti...
Embodiment 2
[0075] 1. Feeding: according to the proportion of the formula, feed the material with a total amount of 1000g coupling agent, namely:
[0076]
[0077] 2. Preparation method:
[0078] 1) Weighing various ingredients according to the prescription quantity;
[0079] 2) Add 7.0g of carbomer into 400g of deionized water, stir in a water bath at 50-68°C until completely dissolved, and leave it;
[0080] 3) 5.0 g of 20% polyhexamethylene biguanide is completely dissolved in 50.0 g of glycerol, and left in place;
[0081] 4) chloramphenicol 2.5g is completely dissolved in 50g of propylene glycol, and left;
[0082] 5) Dissolve 2g of sodium hydroxide weighed in 100g of deionized water completely, and leave
[0083] 6) Mix the mixed solution obtained in step 3) and 4) evenly, then add to the carbomer solution obtained in step 2) and stir until uniform, then add the remaining deionized water, and slowly add sodium hydroxide solution under stirring Stir until uniform, make a neutr...
Embodiment 3
[0086] 1. Feeding: according to the proportion of the formula, feed the material with a total amount of 1000g coupling agent, namely:
[0087]
[0088] 2. Preparation method:
[0089] 1) Weighing various ingredients according to the prescription quantity;
[0090] 2) Add Carbomer 9.0 to 400g of deionized water, stir in a water bath at 50-68°C until completely dissolved, and leave it;
[0091] 3) 2.5 g of 20% polyhexamethylene biguanide is completely dissolved in 70.0 g of glycerol, and left in place;
[0092] 4) Dissolve 2.0 g of chloramphenicol completely in 70 g of propylene glycol and leave it there;
[0093] 5) Dissolve the 2.5g sodium hydroxide taken by weighing in 100g deionized water completely, leave
[0094] 6) Mix the mixed solution obtained in step 3) and 4) evenly, then add to the carbomer solution obtained in step 2) and stir until uniform, then add the remaining deionized water, and slowly add sodium hydroxide solution under stirring Stir until uniform, ma...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com