A production method and technology of oil decoration, which are applied in the fields of technology for producing decorative surface effects, decorative arts, polyester coatings, etc., can solve the problems of no freshness of patterns, poor three-dimensional effect of products, lack of freshness, etc., and achieve Satisfy visual pursuit, strong three-dimensional effect and good sensitivity

Inactive Publication Date: 2010-09-15
刘锋
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, such simulated marble has mainly lines or irregular textures, and the three-dimensional effect is poor.
[0004] In addition, fritillary stone based on unsaturated resin has also appeared. The flower shape of this product is like bean curd residue, which lacks freshness; the colorful pattern based on unsaturated resin has a flower shape slightly similar to that of popcorn oil. (Phoenix stone), but its three-dimensional effect is extremely poor, and the pattern is not vivid

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0033] A preparation method of popcorn oil veneer, which comprises the following preparation steps:

[0034] (1) Fully stir the unsaturated resin, accelerator, paint thinner, colorant and pearlescent product, store for 1 hour, let all the materials fully dissolve, and obtain the resin oil;

[0035] (2) Add the resin oil to the curing agent and stir quickly evenly, then evenly spread the stirred resin oil on the surface of the object to be made, and then evenly spread the diffusing agent on the tiled oil surface according to the size of the pattern to be made , to be solidified;

[0036] (3) Grinding: Use 80°C on the thoroughly cured oil surface # Use sandpaper to thoroughly polish the surface on the oil surface, and then use 240 # Sandpaper will sand the sand marks on the sanding surface;

[0037] (4) Polishing oil: remove the dust on the surface of the polished object, then add the unsaturated resin to the accelerator, curing agent, and liquid wax, stir evenly, and then ap...

Embodiment 2

[0057] A preparation method of popcorn oil veneer, which comprises the following preparation steps:

[0058] (1) Fully stir unsaturated resin, accelerator, paint thinner, colorant, pearlescent products and reflective powder, and store for 10 hours to fully dissolve all materials to obtain resin oil;

[0059] (2) Add the resin oil to the curing agent and stir quickly evenly, then evenly spread the stirred resin oil on the surface of the object to be made, and then evenly spread the diffusing agent on the tiled oil surface according to the size of the pattern to be made , to be solidified;

[0060] (3) Grinding: Use 80°C on the thoroughly cured oil surface # Sandpaper the surface layer on the oil surface thoroughly polished, and then use 240 # Sandpaper will sand the sand marks on the sanding surface;

[0061] (4) Polishing oil: remove the dust on the surface of the polished object, then add the unsaturated resin to the accelerator, curing agent, and liquid wax, stir evenly, ...

Embodiment 3

[0081] A preparation method of popcorn oil veneer, which comprises the following preparation steps:

[0082] (1) Fully stir the unsaturated resin, accelerator, paint thinner, colorant, pearlescent product, and fluorescent powder evenly, store for 24 hours, let all the materials fully dissolve, and obtain the resin oil;

[0083] (2) Add the resin oil to the curing agent and stir quickly evenly, then evenly spread the stirred resin oil on the surface of the object to be made, and then evenly spread the diffusing agent on the tiled oil surface according to the size of the pattern to be made , to be cured;

[0084] (3) Grinding: Use 80°C on the thoroughly cured oil surface # Use sandpaper to thoroughly polish the surface on the oil surface, and then use 240 # Sandpaper will sand the sand marks on the sanding surface;

[0085] (4) Polishing oil: remove the dust on the surface of the polished object, then add the unsaturated resin to the accelerator, curing agent, and liquid wax,...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to a manufacturing method of a puffing paint decorative surface, belonging to the technical field of furniture materials. The manufacturing method comprises the following steps of: (1) sufficiently uniformly stirring unsaturated resin, a promoter, a paint diluent, a colorant and a pearlescent product, and placing for 1-24 hours to sufficiently dissolve all the materials so as to obtain resin oil; (2) fast uniformly stirring the resin oil by adding a curing agent, then uniformly laying the resin oil which is uniformly stirred on the surface of a manufactured article, then uniformly dispersing a diffusant on the laid oil surface in a dripping way according to the size of manufactured patterns, and waiting for curing; (3) burnishing; (4) brushing gloss oil; and (5) grinding with water to obtain a finished product. The manufactured puffing paint decorative surface has the advantages of clear outline, good light sensitivity, strong stereoscopic sensation and high vividness and better meets the visual requirements of people on the luxury of home decorations.

Description

technical field [0001] The invention belongs to the technical field of furniture decorative materials, and in particular relates to a method for making a popcorn oil decorative surface. Background technique [0002] With the improvement of material living standards, people's visual pursuit of luxury home accessories is becoming more and more intense. Because natural materials are difficult to process and engrave, and the price is expensive, there are furniture decorations based on unsaturated resins on the market. material products. [0003] The application number is 00134990.2 Chinese Invention introduces a manufacturing method of simulated marble and simulated marble, including a substrate, a simulation layer is attached to the surface of the substrate, and the raw materials for manufacturing the simulation layer include unsaturated resin gel coat or unsaturated resin glue, curing agent , Accelerator and stone particles, the stone particles are natural or artificial stone...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): B44C1/20C09D167/06C09D7/12
Inventor 傅良明
Owner 刘锋
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products