Coal gangue biomass solid forming fuel and preparation method thereof
A solid briquette fuel, solid fuel technology, applied in solid fuels, biofuels, waste fuels, etc., can solve the problem of wasting the effective thermal components of coal gangue, achieve good social benefits, environmental protection benefits, economic benefits, and stable combustion calorific value. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] After pulverizing 400kg (weight percent: 40%) of coal gangue with a calorific value higher than 2000 kcal, mix it with 500kg (weight percent: 50%) of Eupatorium adenophorum, water hyacinth, weed stems, One or more agricultural organic wastes in crop stalks, peanut shells, grain bran, wheat bran, sawdust, edible fungus residue, and 50kg (weight percentage: 5%) selected from salt, lime, calcium carbonate , heavy oil, sodium nitrate, potassium permanganate, sodium carbonate, potassium oxide, sodium nitrite, sodium hypochlorite, magnesium carbonate, one or more combustion aids, and 50kg (% by weight: 5%) of clay and The binder of polyvinyl alcohol is mixed evenly to obtain a mixture, and then the mixture is made into a granular, columnar, spherical, block or rod-shaped solid material through a molding machine, and finally dried naturally, screened, and measured for packaging.
Embodiment 2
[0032] After pulverizing 600kg (weight percent: 60%) of coal gangue with a calorific value higher than 2000 kcal, mix it with 350kg (weight percent: 35%) of Eupatorium adenophorum, water hyacinth, weed stems, One or more agricultural organic wastes in crop stalks, peanut hulls, grain bran, wheat bran, sawdust, edible fungus residue, and 25kg (weight percentage: 2.5%) selected from salt, lime, calcium carbonate , heavy oil, sodium nitrate, potassium permanganate, sodium carbonate, potassium oxide, sodium nitrite, sodium hypochlorite, magnesium carbonate, one or more combustion accelerants, and 25kg (weight percent: 2.5%) selected from clay and The binder of polyvinyl alcohol is mixed evenly to obtain a mixture, and then the mixture is made into a granular, columnar, spherical, block or rod-shaped solid material through a molding machine, and finally dried naturally, screened, and measured for packaging.
Embodiment 3
[0034] After pulverizing 850kg (weight percentage: 85%) of coal gangue with a calorific value higher than 2000 kcal, mix it with 100kg (weight percentage: 10%) of Eupatorium adenophorum, water hyacinth, weed stems, One or more agricultural organic wastes in crop stalks, peanut shells, grain bran, wheat bran, sawdust, edible fungus residue, and 40kg (weight percentage: 4%) selected from salt, lime, calcium carbonate , heavy oil, sodium nitrate, potassium permanganate, sodium carbonate, potassium oxide, sodium nitrite, sodium hypochlorite, magnesium carbonate, one or more combustion accelerants, and 10kg (percentage by weight: 1%) selected from clay and The binder of polyvinyl alcohol is mixed evenly to obtain a mixture, and then the mixture is made into a granular, columnar, spherical, block or rod-shaped solid material through a molding machine, and finally dried naturally, screened, and measured for packaging.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com