Sealing corrosion-resistant structure of expansion joint of brick lining chimney
An expansion joint and lining technology, which is applied in building components, building insulation materials, building types, etc., can solve problems such as difficulty in handling expansion joints and leakage, and achieve good long-term sealing function, good sealing effect and good sealing performance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0013] Such as figure 1 As shown, it is a sectional view of a brick-lined chimney expansion joint sealing and anti-corrosion structure provided by the present invention, which is applied on the chimney outer cylinder 1, and between the chimney outer cylinder 1 and the chimney brick lining 3 is a sealed air or heat insulation layer 2. According to the actual matrix condition, the brick 12 can also be added later. The purpose of adding this brick is to adjust the size of the expansion joint reserved under the drip plate 9. The joint should be less than 80mm. Sealing material for chimney gaps13. After cleaning or sandblasting of all brick lining surfaces, paint epoxy primer (such as Henkel's PENNTROWEL EPOEXY primer) 4, fill the reserved seam under the drip board 9 with compressible rock wool 11, and use elastic glue Adhesive (such as Henkel PENNGUARD ADHESIVE MEMBRANE) 5 coated surface and brick surface seal. The sealing film 8 is fixed on the facade of the upper brick and the...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com