A nano-bamboo charcoal, antibacterial fiber technology, applied in the manufacture of rayon, fiber chemical characteristics, melt spinning and other directions, can solve the problems of antibacterial agent shedding, harm, reduction of antibacterial effect, etc., and achieve excellent antibacterial and wide-ranging effects.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] Add 8 kg of nano bamboo charcoal powder and 2 kg of nano silver powder to 40 kg of polyester chips. According to the preparation method of nano bamboo carbon antibacterial fiber masterbatch, the mixing temperature is 270 ℃, the internal pressure of the extruder is 7.5 MPa, and the twin screw is used. It is extruded and granulated by a machine to produce nano bamboo carbon antibacterial fiber masterbatch.
[0033] Add the 50 kg nano-bamboo-carbon antibacterial fiber masterbatch to 250 kg of polyester chips to mix, and draw the desired nano-bamboo-carbon antibacterial polyester fiber product according to the above-mentioned melt-spinning method. The mass fraction of nano bamboo charcoal powder in the nano bamboo charcoal antibacterial polyester fiber is 2.66%, and the mass fraction of nano silver powder is 0.66%.
Embodiment 2
[0035] Add 3 kg of nano bamboo charcoal powder and 1 kg of nano silver powder to 20 kg of polypropylene fiber slices. According to the preparation method of the above-mentioned nano bamboo carbon antibacterial fiber masterbatch, the mixing temperature is 265°C, the extruder pressure is 7Mpa, and it is extruded by a twin screw. Machine granulation, made into nano bamboo carbon antibacterial fiber masterbatch.
[0036] The above 24 kilograms of nano bamboo carbon antibacterial fiber masterbatch is added to 76 kilograms of polypropylene fiber slices and mixed, and then melt-spinned to produce the required nano bamboo carbon antibacterial (polypropylene) fiber. The mass fraction of nano bamboo charcoal powder in the nano bamboo charcoal antibacterial (polypropylene) fiber is 3%, and the mass fraction of nano silver is 1%.
Embodiment 3
[0038] Add 6 kg of nano bamboo charcoal powder and 2 kg of nano silver powder to 20 kg of nylon chips. According to the preparation method of the above-mentioned nano bamboo carbon antibacterial fiber masterbatch, the mixing temperature is 260 ℃, the extruder pressure is 7Mpa, and the extruder is extruded by a twin screw. Press granulation to produce nano bamboo carbon antibacterial fiber masterbatch.
[0039] The above 28 kilograms of nano bamboo carbon antibacterial fiber masterbatch is added to 72 kilograms of nylon chips and mixed, and then melted and spun to make the required nano bamboo carbon antibacterial (nylon) fiber. The mass fraction of nano bamboo charcoal powder in the nano bamboo charcoal antibacterial (nylon) fiber is 6%, and the mass fraction of nano silver is 2%.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
quality score | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com