Rolling oil composition for 12-roller reversing mill
A rolling oil and composition technology, applied in lubricating compositions, petroleum industry, base materials, etc., can solve problems such as inconvenient use, affecting the cleanliness of rolling mills, failing to meet the use requirements, etc., and achieve obvious economic and social benefits, The effect of significant technological advancement and outstanding features
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0061] Add 9.6g of 150SN mechanical oil and 9.6g of 500SN mechanical oil to the blending kettle, raise the temperature to 60-70°C, add 1.5g of antioxidant 2,6-di-tert-butyl p-cresol, and copolymerize defoamer acrylate and ether T911 10.1g, stir until the additive dissolves; cool down to 60°C, add 25g of pentaerythritol oleic acid, stearic acid, dimer acid mixed ester, trimethylolpropane coconut oleic acid, palmitoleic acid, oleic acid 40g of mixed acid ester, stir evenly; at 50°C, add 2g of phosphorus-containing extreme pressure antiwear agent C12 fatty alcohol polyoxyethylene ether (3) phosphate ester, 1.2g of rust inhibitor cyclohexylamine, stir for 30 minutes, and finally add 16 g of emulsifier Pluronic L1, 4 g of Tween-80, and 1 g of sulfurized olefinic cottonseed oil T405A, a sulfur-containing extreme pressure and anti-wear agent, were stirred for 30 minutes to obtain 100 g of the composition of the present invention.
Embodiment 2
[0063] Add 6.4g of 25# transformer oil and 12g of 500SN mechanical oil to the blending kettle, raise the temperature to 60-70°C, add 1g of antioxidant 2,6-di-tert-butyl-p-cresol, N-phenyl-a-naphthylamine 0.5g, defoamer acrylate and ether copolymer T911 0.1g, stir until the additive is dissolved; cool down to 60°C, add pentaerythritol oleic acid, stearic acid, dimer acid mixed ester 20g, trimethylolpropane 45g of mixed esters of coconut oleic acid, palmitoleic acid and oleic acid, and stir evenly; at 50°C, add 2g of phosphorus-containing extreme pressure antiwear agent C12 fatty alcohol phosphate, and 1.5g of rust inhibitor cyclohexylamine, and stir After 30 minutes, 5.5 g of emulsifier Pluronic L121, 5.5 g of NP-10, and 0.5 g of sulfurized isobutylene T321, a sulfur-containing extreme pressure antiwear agent, were added, and stirred for 30 minutes to obtain 100 g of the composition of the present invention.
Embodiment 3
[0065] Add 7.6g of 40# transformer oil and 7.6g of 500SN mechanical oil to the blending kettle, raise the temperature to 60-70°C, add 1g of antioxidant 2,6-di-tert-butyl-p-cresol, N-phenyl-a-naphthalene Amine 1g, defoamer acrylate and ether copolymer T911 0.1g, stir until the additive is dissolved; cool down to 60°C, add pentaerythritol oleic acid, stearic acid, dimer acid mixed ester 33g, trimethylolpropane 35g of mixed acid ester of coconut oil and oleic acid, stir evenly; at 50°C, add phosphorus-containing extreme pressure antiwear agent C12 fatty alcohol polyoxyethylene ether (9) phosphate ester 1.5g, and rust inhibitor cyclohexylamine 0.7g, stirred for 30 minutes, finally added 6g of emulsifier Pluronic L121, 5g of NP-10, and 1.5g of vulcanized lard, a sulfur-containing extreme pressure antiwear agent, stirred for 30 minutes to obtain 100g of the composition of the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com