Embodiment 1
[0052] Take 42 parts (weight) of polyester acrylate, add 5 parts (weight) of epoxy acrylate, 20 parts (weight) of high-viscosity monofunctional urethane acrylate, 3 parts (weight), 10 parts (weight) of photoinitiator, disperse at high speed, stir evenly, until the photoinitiator is completely dissolved. Under the condition that the rotation speed of the mixer is less than 300 r / min, 4 parts (weight) of filler and 16 parts (weight) of yellow organic pigment are put in. After the materials are evenly mixed, under the condition that the speed of the mixer is >600r / min, disperse at a high speed, fully wet the powder, and then grind it with a three-roller machine to a fineness of ≤6um to obtain the finished product.
Embodiment 2
[0054] Take 42 parts (weight) of polyester acrylate, add 5 parts (weight) of epoxy acrylate, 20 parts (weight) of high-viscosity monofunctional urethane acrylate, 3 parts (weight), 10 parts (weight) of photoinitiator, disperse at high speed, stir evenly, until the photoinitiator is completely dissolved. When the speed of the mixer is less than 300 r / min, 4 parts (weight) of filler and 16 parts (weight) of red organic pigment are put in. After the materials are evenly mixed, under the condition of the mixer speed > 600r / min, disperse at high speed to fully wet the powder. Then use a three-roller to grind to a fineness of ≤6um, and the finished product is obtained.
Embodiment 3
[0056] Take 42 parts (weight) of polyester acrylate, add 5 parts (weight) of epoxy acrylate, 20 parts (weight) of high-viscosity monofunctional urethane acrylate, 3 parts (weight), 10 parts (weight) of photoinitiator, disperse at high speed, stir evenly, until the photoinitiator is completely dissolved. When the speed of the mixer is less than 300 r / min, 4 parts (weight) of filler and 16 parts (weight) of blue organic pigment are put in. After the materials are evenly mixed, under the condition of the mixer speed > 600r / min, disperse at high speed to fully wet the powder. Then use a three-roller to grind to a fineness of ≤6um, and the finished product is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com