Preparation of low free monomer, degradable persimmon tannin modified phenolic resin
A phenolic resin, low free technology, applied in the field of preparation of modified phenolic resin to reduce pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] Take 28.5g of phenol and 8g of persimmon tannin solution (mass concentration of tannin≥3wt%), add them into a reaction vessel equipped with a reflux condenser and an electric stirrer, stir evenly and add 0.85g of oxalic acid. The temperature was raised to 90° C., and 15.5 g of formaldehyde solution was added dropwise (the mass concentration of formaldehyde in the formaldehyde solution was 38%, at this time, the molar ratio of formaldehyde to phenol was 0.64). After 50 minutes, the formaldehyde solution was added dropwise. Then heat to 95°C to reflux the reactants for 60 minutes, depressurize (pressure 0.04Mpa) for dehydration, stop dehydration when the viscosity of the resin reaches 110cPa.s, cool down to 30°C and collect the materials to obtain low free monomer and degradable Persimmon tannin modified phenolic resin. The test results of the obtained resin are shown in Table 1.
Embodiment 2
[0023] Take 28.5g of phenol and 14g of persimmon tannin solution (mass concentration of tannin≥3wt%), add them into a reaction vessel equipped with a reflux condenser and an electric stirrer, stir evenly and add 0.85g of oxalic acid. The temperature was raised to 95° C., and 24.85 g of formaldehyde solution was added dropwise (the mass concentration of formaldehyde in the formaldehyde solution was 39%, and at this time, the molar ratio of formaldehyde to phenol was 1.06). After 60 minutes, the formaldehyde solution was added dropwise. Reheat to 95°C and react for 70 minutes, then dehydrate under reduced pressure (pressure is 0.03Mpa), stop dehydration when the viscosity of the resin reaches 200cPa.s, cool down to 30°C and collect materials, and obtain low free monomer, degradable persimmon tannin Modified phenolic resin. The test results of the obtained resin are shown in Table 1.
Embodiment 3
[0025] Get 28.2g of phenol, 14g of persimmon tannin solution (mass concentration of tannin ≥ 3wt%), add in the reaction vessel that reflux condenser, electric stirrer are housed, after stirring evenly, add the hydrochloric acid 0.5g that mass concentration is 20%. The temperature was raised to 95° C., and 20.62 g of formaldehyde solution was added dropwise (the mass concentration of formaldehyde in the formaldehyde solution was 39%, and at this time, the molar ratio of formaldehyde to phenol was 0.89). After 60 minutes, the formaldehyde solution was added dropwise. Reheat to 95°C and react for 70 minutes, dehydrate under reduced pressure (pressure is 0.05Mpa), stop dehydration when the viscosity of the resin reaches 300cPa.s, cool down to 30°C and collect the material, and obtain low free monomer, degradable persimmon tannin Modified phenolic resin. The test results of the obtained resin are shown in Table 1.
PUM
![No PUM](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com