Method for preparing smoke treating and water source purifying double-purpose active coke and products thereof
A technology of active coke and water source, applied in chemical instruments and methods, other chemical processes, etc., can solve the problems of narrow application range and strong specificity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Crush 55 kg of coke powder, 15 kg of coking coal and 5 kg of anthracite into coal powder with more than 90% passing through a 200-mesh screen, heat and melt the pitch, stir it evenly, and keep it warm for later use; add molten pitch to the coal powder, the amount Add 10 parts by weight for every 100 parts by weight of coal powder. After kneading evenly, send it to a double-roll molding machine with a pressure of 50.0 MPa, and press it into φ10mm spherical particles; then send the spherical particles to a carbonization furnace at 750°C for carbonization After hours, the carbonized material is made into carbonized material; then the carbonized material is sent into a vertical activation furnace, and activated with 0.25MPa water vapor at 950°C for 4 hours to make a dual-purpose activated coke product for flue gas treatment and water source purification.
Embodiment 2
[0028] Crush 60 kg of carbonized powder, 25 kg of 1 / 3 coking coal, and 10 kg of bituminous coal into pulverized coal that can pass through a 200-mesh sieve for more than 90%, heat, melt, mix pitch and tar at a ratio of 20:80, and stir evenly Insulation for standby; add the mixture of molten pitch and tar to the coal powder, the addition amount is 25 parts by weight for every 100 parts by weight of coal powder, after kneading evenly, send it to the double-roll forming machine with a pressure of 180.0MPa, and press it into φ11 ×8mm apricot core-shaped particles; then put the apricot core-shaped particles into a carbonization furnace at 800°C and carbonize for 1.5 hours to make carbonized material; then send the carbonized material into a vertical activation furnace at 980°C with 0.6 Activated by MPa water vapor for 12 hours to make dual-purpose activated coke products for flue gas control and water source purification.
Embodiment 3
[0030] 65 kg of pulverized coal, 30 kg of coking coal and 15 kg of anthracite are respectively crushed into pulverized coal that more than 90% can pass through a 200-mesh sieve, and the asphalt and tar are heated, melted and mixed in a ratio of 30:70, stirred evenly, and kept warm for later use; Add a mixture of molten pitch and tar to the pulverized coal in an amount of 30 parts by weight for every 100 parts by weight of pulverized coal. After kneading evenly, send it to a double-roll molding machine with a pressure of 300.0MPa, and press it into φ13×11×8mm Olive-shaped particles; then send the spherical particles into a carbonization furnace at 780°C, and carbonize for 1.5 hours to make carbonized material; then send the carbonized material into a vertical activation furnace, and activate it with 0.5MPa water vapor at 1050°C for 20 Hours, to make dual-purpose activated coke products for flue gas control and water source purification.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com