Construction method for rubber grain asphalt concrete pavement
A technology of asphalt concrete and rubber granules, which is applied to cohesive pavement paved on site, roads, roads, etc. It can solve the problems of poor steering operation stability, reduced adhesion coefficient, poor wear resistance, etc., to prolong service life and drive Effects of improved comfort and enhanced wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment approach 1
[0006] Specific embodiment one: the construction method of the rubber particle asphalt concrete pavement of the present embodiment is finished like this: a, mixing: first select following raw material and form according to weight percentage: ore aggregate 76.5~91.5%, asphalt 2.5~7.5%, ore powder 4-10%, rubber granules 2-6%, heat the ore to 190-200°C, add the rubber granules to the ore and dry mix for 20-25s, then mix the pre-heated asphalt with Mineral powder is added to rubber granules and mineral material for mixing, and the heating temperature of the asphalt is 155-180°C; the entire mixing time from the dry mixing of mineral material and rubber granules to the addition of asphalt and mineral powder is 70-80s. Asphalt mixture; b. Paving: the temperature of the asphalt mixture during paving is 140-175°C, and the loose paving coefficient after paving is 1.25-1.30; c. The first stage of initial pressure: rolling with a road roller, rolling The temperature of the asphalt mixture...
specific Embodiment approach 2
[0007] Embodiment 2: The difference between this embodiment and Embodiment 1 is that in this embodiment, in the mixing step a, the particle diameter of the rubber particles is 0.3-5 mm. It can improve the elastic deformation characteristics and surface state of the mixture.
specific Embodiment approach 3
[0008] Specific embodiment 3: The difference between this embodiment and specific embodiment 1 is: In this embodiment, in the initial compaction step of the first stage c, a 10-12t double-wheel steel drum roller is used for rolling twice. In order to reduce the occurrence of wheel sticking caused by the high-viscosity characteristics of the material, it is advisable to use a double-wheel steel drum roller for rolling when the temperature is high.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com