[0021] The composition of gold paint includes acrylic acid, aluminum powder, yellow complex dye, orange complex dye, gold powder, ultraviolet absorber, ethyl acetate, aluminum powder orientation agent, anti-settling agent, butyl acetate cellulose, and their The ratio is: acrylic acid 52.937%, aluminum powder 5.263%, yellow complex dye 1.1%, orange complex dye 1.9%, gold powder 1.2%, UV absorber 1.8%, ethyl acetate 22.34%, propylene glycol methyl ether acetate 10%, aluminum powder orientation agent 0.4%, anti-settling agent 0.6%, butyl acetate cellulose 2.46%.
[0022] The production process of gold paint includes the following steps: soaking 22.34% ethyl acetate and 5.263% aluminum powder for 35 minutes; 52.937% acrylic acid and 5.263% aluminum powder orientation agent, 0.6% aluminum powder Anti-settling agent and 1.2% gold powder are dispersed at high speed at 1000 rpm to make pulp; 10% propylene glycol methyl ether acetate and 2.46% butyl acetate cellulose are mixed at high ...
Embodiment 2
[0024] The composition of gold paint includes alkyd, copper powder, yellow complex dye, orange complex dye, gold powder, ultraviolet absorber, butyl acetate, copper powder orienting agent, anti-settling agent, butyl acetate cellulose, etc. The ratio of alkyd is 55.621%, copper powder 5.144%, yellow complex dye 1.5%, orange complex dye 2.5%, gold powder 0.8%, UV absorber 1.5%, butyl acetate 20.055%, propylene glycol methyl ether Acetate 9%, copper powder orientation agent 0.5%, anti-settling agent 0.5%, butyl acetate cellulose 2.88%.
[0025] The production process of the gold paint includes the following steps: soaking 20.055% butyl acetate and 5.144% copper powder for 40 minutes; 55.621% two-thirds of the alkyd and 0.5% copper powder orientation agent, 0.5% Anti-settling agent, 0.8% gold powder were dispersed at high speed at 1000 rpm to make pulp; 9% propylene glycol methyl ether acetate and 2.88% butyl acetate cellulose were mixed at 1000 rpm Disperse at high speed to make...
Embodiment 3
[0027] The composition of gold paint includes polyester, pearl powder, yellow complex dye, orange complex dye, gold powder, ultraviolet absorber, butyl acetate, pearl powder orientation agent, anti-settling agent, butyl acetate cellulose, which are The ratio is: polyester 57.892%, pearl powder 5.644%, yellow complex dye 1.7%, orange complex dye 2.6%, gold powder 0.9%, UV absorber 1.2%, butyl acetate 19.164%, propylene glycol methyl ether Acetate 7%, pearlescent powder orientation agent 0.6%, anti-settling agent 0.4%, butyl acetate cellulose 2.9%.
[0028] The production process of gold paint includes the following steps: soaking 19.164% butyl acetate and 5.644% pearl powder for 45 minutes; 57.892% polyester and 0.6% pearl powder orientation agent, 0.4% Anti-settling agent, 0.9% gold powder were dispersed at high speed at 1000 rpm to make pulp; 7% propylene glycol methyl ether acetate and 2.9% butyl acetate cellulose were mixed at 1000 rpm Disperse at high speed to make a slur...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com