Oxidation process of preparing wool keratin solution

A protein solution and oxidation technology, applied in the field of preparation of wool keratin solution, can solve the problems of high dissolving temperature, inability to maintain wool physical and chemical properties, low solubility, etc.

Inactive Publication Date: 2007-06-27
ZHEJIANG HAPPY CHEM
View PDF0 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0009] This method mainly dissolves at a high temperature, so that the prepared solution cannot maintain the original physical and chemical properties of wool, and has defects such as low solubility. This problem has become a difficult problem to be solved urgently.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Oxidation process of preparing wool keratin solution

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0022] Embodiment 1: wool is washed with the sodium lauryl sulfate solution of concentration 4%, the bath ratio of wool and this solution is 1: 40, temperature 70 ℃, time 30min, and wash under the condition of stirring; H 2 o 2 Add urea under stirring, and H 2 o 2 The weight ratio of urea and urea is 3: 4, keep the temperature at 30 DEG C, stir and react for 1.5 hours to obtain urea hydrogen peroxide adduct; mix the urea hydrogen peroxide adduct obtained above with distilled water, and the process The weight ratio of urea hydrogen oxide adduct to distilled water is 1:1, and anionic surfactant is added under stirring state, under normal temperature state, stirring for 1 hour, a colorless transparent liquid is obtained; the colorless transparent liquid prepared above is put into Add the wool obtained above, the weight ratio of the liquid to the wool is 5: 1, keep stirring, and slowly heat up to 65°C, after 6 hours, a light yellow translucent liquid is obtained, and the insolub...

Embodiment 2

[0023] Embodiment 2: wool is washed with the sodium lauryl sulfate solution of concentration 4%, the bath ratio of wool and this solution is 1: 30, temperature 60 ℃, time 40min, and wash under the condition of stirring; H 2 o 2 Add urea under stirring, and H 2 o 2 The weight ratio of urea and urea is 3: 4, keep the temperature at 26 ° C, and stir for 1.5 hours to obtain urea hydrogen peroxide adduct; the above-mentioned urea hydrogen peroxide adduct prepared above is mixed with distilled water, and the process The weight ratio of urea hydrogen oxide adduct to distilled water is 14:10, and anionic surfactant is added under stirring state, under normal temperature state, stirring for 1 hour, a colorless transparent liquid is obtained; the colorless transparent liquid prepared above is put into Add the wool obtained above, the weight ratio of the liquid to the wool is 10:1, keep stirring, and slowly heat up to 70°C, after 5 hours, a light yellow translucent liquid is obtained, ...

Embodiment 3

[0024] Embodiment 3: wool is washed with the sodium lauryl sulfate solution of concentration 4%, the bath ratio of wool and this solution is 1: 50, temperature 68 ℃, time 40min, and wash under the condition of stirring; H 2 o 2 Add urea under stirring, and H 2 o 2 The weight ratio of urea and urea is 3: 4, keep the temperature at 30 DEG C, stir and react for 1.5 hours to obtain urea hydrogen peroxide adduct; mix the urea hydrogen peroxide adduct obtained above with distilled water, and the process The weight ratio of urea hydrogen oxide adduct to distilled water is 14:15, and an anionic surfactant is added under stirring state, under normal temperature state, stirring for 1 hour, a colorless transparent liquid is obtained; the colorless transparent liquid prepared above is put into Add the wool obtained above, the weight ratio of the liquid to the wool is 20: 1, keep stirring, and slowly heat up to 85°C, after 4 hours, a light yellow translucent liquid is obtained, and the i...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The present invention discloses oxidation process of preparing wool keratin solution, and the preparation process can maintaining the physical and chemical performance of wool and has raised solubility and lowered wool dissolving temperature. The preparation process includes the following steps: washing and stoving wool; preparing wool dissolving solution through adding urea into H2O2 to obtain adduct, mixing the adduct with distilled water and adding anionic surfactant via stirring to obtain transparent liquid as the wool dissolving solution; mixing wool dissolving solution and wool in the weight ratio of 5-20 to 1 via stirring, heating to 65-85 deg.c and maintaining for 4-6 hr to obtain yellowish translucent liquid and filtering to eliminate insoluble impurity and obtain wool keratin solution. The process is simple and low in cost.

Description

technical field [0001] The invention relates to a method for preparing a wool keratin protein solution, in particular to a method for preparing a wool keratin protein solution by an oxidation method. Background technique [0002] The regeneration and utilization of natural protein fibers has become a hot issue nowadays, and has attracted the attention of researchers from all walks of life, and the regeneration and utilization of wool keratin protein is the most active field of research. After the waste wool is dissolved, it is prepared into wool keratin protein solution, which can be processed into fibers of various specifications by artificial spinning technology, and can also be used as a finishing agent for textiles, endowing other textiles with the physical and chemical properties of wool fibers . The prepared wool keratin protein solution is also widely used in hair care, skin care products and nutritional additives for animal feed. At present, there are two main ways...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C07K1/12C07K1/14C07K2/00
Inventor 雷志涛陶海峰孙超沈丽丽
Owner ZHEJIANG HAPPY CHEM
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products