[0011] As shown in the manufacturing method of this self-cleaning anti-fog glass, the titanium sol used is composed of butyl titanate, ethanol, triethanolamine and water, and is composed of butyl titanate: ethanol: triethanolamine: water =20:75:5:1~3 ratio.
[0012] In the specific preparation of titanium sol, the above three chemical raw materials should be stirred together for 1 to 2 hours, then deionized water according to the preparation amount should be added to it, and the stirring should be continued for 0.5 to 1 hour, so that they can be fully mixed. uniform state, and the sol was allowed to stand for 8 to 24 hours, and thus the preparation of the suitable titanium sol was completed.
[0013] The pretreatment of the coated glass is to pickle and soak the glass to be coated by chemical and physical methods, and then clean it with ethanol and deionized water and dry it;
[0014] The drying of the coating film means that the above-mentioned glass is immersed in the prepa...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com