Embodiment 1
[0021] The production process of the negative ion sponge machine foaming line used for upholstered furniture includes the following steps:
[0022] Step 1: raw material preparation, take 98% of polyether polyol, 40% of organic isocyanate, 3% of natural water, 4% of methane, 150% of negative ion additive, 0.35% of stannous octoate, and 0.2% of ethanolamine in parts by mass for standby;
[0023] Step 2: Add polyether polyol, organic isocyanate, natural water, methane, stannous octoate, and ethanolamine into a small material stirring mixer with heating function and stir for 10 minutes, and ensure that the temperature of the material is 25°C;
[0024] Step 3: Add the anion additive to the mixture in the step 2 and add it into a large-material stirring mixer with heating function to stir for 20 minutes, and ensure that the material temperature is at 25°C;
[0025] Step 4: Adjust the height of the six drop boards as needed;
[0026] Step 5: Confirm that the milky white reaction tim...
Embodiment 2
[0029] The production process of the negative ion sponge machine foaming line used for upholstered furniture includes the following steps:
[0030] Step 1: raw material preparation, take 98% of polyether polyol, 40% of organic isocyanate, 3% of natural water, 4% of methane, 150% of negative ion additive, 0.35% of stannous octoate, and 0.2% of ethanolamine in parts by mass for standby;
[0031] Step 2: Add polyether polyol, organic isocyanate, natural water, methane, stannous octoate, and ethanolamine into a small material stirring mixer with heating function and stir for 15 minutes, and ensure that the temperature of the material is at 22°C;
[0032] Step 3: Add the anion additive to the mixture in the step 2 and add it into a large-material stirring mixer with heating function to stir for 20 minutes, and ensure that the material temperature is at 25°C;
[0033] Step 4: Adjust the height of the six drop boards as needed;
[0034] Step 5: Confirm that the milky white reaction ...
Embodiment 3
[0037] The production process of the negative ion sponge machine foaming line used for upholstered furniture includes the following steps:
[0038] Step 1: raw material preparation, take 98% of polyether polyol, 40% of organic isocyanate, 3% of natural water, 4% of methane, 150% of negative ion additive, 0.35% of stannous octoate, and 0.2% of ethanolamine in parts by mass for standby;
[0039] Step 2: Add polyether polyol, organic isocyanate, natural water, methane, stannous octoate, and ethanolamine into a small material stirring mixer with heating function and stir for 10 minutes, and ensure that the temperature of the material is 25°C;
[0040] Step 3: Add the anion additive to the mixture in the step 2 and add it into a large-material stirring mixer with heating function to stir for 15 minutes, and ensure that the material temperature is at 26°C;
[0041] Step 4: Adjust the height of the six drop boards as needed;
[0042] Step 5: Confirm that the milky white reaction tim...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com