Preparation method of side chain hydrophilically-modified block silicone oil for cotton
A technology of block silicone oil and hydrophilic modification, applied in the direction of improved hand-feeling fibers, textiles and papermaking, fiber processing, etc., can solve the problems of inability to meet diversified handfeel, unsatisfactory washing resistance, poor fabric handfeel, etc. , to achieve the effect of improving the hydrophilic ability, improving the washing resistance and improving the hand feeling.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0013] Example 1: 100 grams of side chain hydrogen-containing silicone oil with a number average molecular weight of 6000, 35 grams of allyl epoxy polyether with a number average molecular weight of 300, and 55 grams of isopropanol are added to a reaction vessel equipped with a condensation reflux device In the process, the temperature of the reaction vessel was raised to 78°C, 0.005 g of chloroplatinic acid was added, and the reaction was carried out at 80°C for 2 hours to obtain a side chain polyether epoxy silicone oil, the temperature was lowered to 20°C, and 37 g of double-ended polyether with a number average molecular weight of 300 was added. Aminopolyethylene glycol, 1.5 g of glycidyl cage silsesquioxane, heating the reaction vessel to 81° C., and keeping it warm for 9 hours to prepare side chain hydrophilic modified block silicone oil for cotton.
Embodiment 2
[0015] 100 grams of side chain hydrogen-containing silicone oil with a number average molecular weight of 8000, 40 grams of allyl epoxy polyether with a number average molecular weight of 400, and 60 grams of isopropanol were added to a reaction vessel equipped with a condensation reflux device, and the reaction vessel Raise the temperature to 79°C, add 0.007 g of chloroplatinic acid, and keep the temperature at 81°C for 3 hours to prepare side chain polyether epoxy silicone oil, cool down to 30°C, add 45 g of double-ended aminopolyethylene glycol with a number average molecular weight of 400 Alcohol, 1.8 grams of glycidyl cage silsesquioxane, the reaction vessel was heated to 83 ° C, and kept for 10 hours for reaction to obtain side chain hydrophilic modified block silicone oil for cotton.
Embodiment 3
[0017] 100 grams of side chain hydrogen-containing silicone oil with a number average molecular weight of 10,000, 50 grams of allyl epoxy polyether with a number average molecular weight of 600, and 65 grams of isopropanol were added to a reaction vessel equipped with a condensation reflux device, and the reaction vessel Raise the temperature to 80°C, add 0.009 g of chloroplatinic acid, and keep the temperature at 81°C for 4 hours to prepare side chain polyether epoxy silicone oil, cool down to 35°C, add 55 g of double-ended aminopolyethylene glycol with a number average molecular weight of 600 Alcohol, 2 grams of glycidyl cage silsesquioxane, the reaction vessel was heated to 85° C., and kept for 12 hours, to obtain side chain hydrophilic modified block silicone oil for cotton.
[0018] Application and finishing process of side chain hydrophilic modified block silicone oil for cotton:
[0019] 1. Preparation of side chain hydrophilic modified block silicone oil emulsion for c...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com