Nano porous starch-based material with high oil absorption rate and preparation method and application thereof
A nanoporous, high oil absorption technology, applied in separation methods, chemical instruments and methods, other chemical processes, etc., to achieve stable structure, high oil absorption effect, and good oil absorption effect.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] A preparation method of nanoporous starch-based material with high oil absorption rate, comprising the following steps:
[0040] 1. Gelatinization treatment of starch: Take 100 g of starch and dissolve it in 10 L of distilled water, gradually raise the temperature to 95°C at a rate of 8°C / min and keep for 2 minutes, then cool to room temperature for later use;
[0041] 2. Add 2 g of calcium carbonate nanoparticles to step 1 and continue to stir for 20 min. Continue to stir overnight at 4°C. Centrifuge at 2500 r / min for 5 min. After washing with water three times, disperse in ethylenediaminetetraacetic acid (0.2 M pH=7.4, EDTA), stirred for 30 min, centrifuged and washed three times with ultrapure water. Repeatedly disperse EDTA, stir, centrifuge and wash;
[0042] Operation points and precautions: Calcium carbonate nanoparticles are dissolved in 10% ethanol water and ultrasonically mixed. When dissolving, ethanol can be added first to dissolve most of the nano-calcium ...
Embodiment 2
[0051] A preparation method of nanoporous starch-based material with high oil absorption rate, comprising the following steps:
[0052] 1. Gelatinization treatment of starch: Take 100 g of starch and dissolve it in 10 L of distilled water, gradually raise the temperature to 95 °C at a rate of 14 °C / min and keep for 4 min, then cool to room temperature for later use;
[0053]2. Add 4 g of calcium carbonate nanoparticles to step 1 and continue to stir for 20 min. Continue to stir overnight at 4°C. Centrifuge at 2500 r / min for 5-10 min. After washing with water three times, disperse in ethylenediamine Tetraacetic acid (0.2M pH=7.4, EDTA), stirred for 30-35 min, and centrifuged and washed three times with ultrapure water. Repeatedly disperse EDTA, stir, centrifuge and wash;
[0054] Operation points and precautions: Calcium carbonate nanoparticles are dissolved in 10% ethanol water and mixed ultrasonically. When dissolving, ethanol can be added first to dissolve most of the nano-...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com