Examples
Embodiment 1
[0011] A cigarette film with uniform thickness, composed of three layers A, B, and C, wherein layer A includes 80 parts by mass of low-volatile copolymer polypropylene, 15 parts by mass of low-volatile slip agent and 7 parts by mass of anti-blocking agent ; B layer includes 65 parts by mass of homopolypropylene, 5 parts by mass of antistatic agent, 30 parts by mass of stiffening agent; layer C includes 94 parts by mass of low-volatile copolymerized polypropylene, 3 parts by mass of low-volatile smooth agent and 3 parts by mass of parts by mass of antiblocking agent.
[0012] The low-volatile copolymerized polypropylene is formed by copolymerizing an elastomer composed of repeating monomers of isotactic polypropylene and randomly distributed ethylene with ethylene and propylene; the low-volatile smooth agent is composed of siloxane and It is compounded with silica, and its molecular weight is 30-50 times that of erucamide slip agents.
Embodiment 2
[0014] A cigarette film with uniform thickness, composed of three layers A, B, and C, wherein layer A includes 90 parts by mass of low-volatile copolymer polypropylene, 10 parts by mass of low-volatile smooth agent and 2 parts by mass of anti-blocking agent ; The B layer includes 98 parts by mass of homopolypropylene, 1 part by mass of antistatic agent, and 1 part by mass of stiffening agent; the layer C includes 97 parts by mass of low-volatile copolymerized polypropylene, 3 parts by mass of low-volatile smooth agent and 3 parts by mass of parts by mass of antiblocking agent.
[0015] The low-volatile copolymerized polypropylene is formed by copolymerizing an elastomer composed of repeating monomers of isotactic polypropylene and randomly distributed ethylene with ethylene and propylene; the low-volatile smooth agent is composed of siloxane and It is compounded with silica, and its molecular weight is 30-50 times that of erucamide slip agents.
Embodiment 3
[0017] A cigarette film with uniform thickness, composed of three layers A, B, and C, wherein layer A includes 86 parts by mass of low-volatile copolymer polypropylene, 14 parts by mass of low-volatile smooth agent and 4 parts by mass of anti-blocking agent ; B layer includes 85 parts by mass of homopolypropylene, 2 parts by mass of antistatic agent, 13 parts by mass of stiffening agent; layer C includes 95 parts by mass of low volatile copolymer polypropylene, 2 parts by mass of low volatile smooth agent and 3 parts by mass parts by mass of antiblocking agent.
[0018] The low-volatile copolymerized polypropylene is formed by copolymerizing an elastomer composed of repeating monomers of isotactic polypropylene and randomly distributed ethylene with ethylene and propylene; the low-volatile smooth agent is composed of siloxane and It is compounded with silica, and its molecular weight is 30-50 times that of erucamide slip agents.
[0019] It can be detected by the inspection m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com