Process for the preparation of stabilized speckled bricks
A spot and stable technology, which is applied in the field of stable spot brick preparation, can solve the problems such as easy flow of spot particles, uneven spot distribution, complicated processing process, etc., and achieve the effect of reducing color and spot dependence and realizing spot and uniform distribution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0025] The present invention will be described in further detail below in conjunction with embodiment:
[0026] The preparation method of this stable spot brick, comprises the following steps:
[0027] ⑴Body pressing: the green body powder is composed of conventional powder and spots; the particle size of regular powder is 0.3-0.6 mm, the particle size of speckled powder is 1-3 mm, and the spots are composed of white, blue and black spots. The proportion of white spots is 8%, the proportion of blue spots is 16%, and the proportion of black spots is 76%;
[0028] ⑵ Body drying: drying temperature 80-130 ℃, drying time 40-60 minutes;
[0029] (3) Simulation treatment: Before pattern decoration, a translucent glaze layer is applied on the surface of the body in advance, and the color of the glaze layer is adjusted to be close to the surface color of the body, and then the inkjet printing decoration technology is used to print out the size and size of the spots on the body. Inkj...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com