Embodiment 1
[0029] A kind of concrete steps of the processing method of cork oak bark yoga column are:
[0030] Step 1: Pick and peel off the fresh bark of the evergreen tree Quercus cork, brush off the moss and impurities on the surface, unfold it while it is wet, stack 15 layers of staggered stacks, and press heavy objects on the stacks;
[0031] Step 2: After the bark of the cork oak becomes flat under the pressure of heavy objects, spread it out in the open air for half a year to dry naturally, and reserve it;
[0032] Step 3: Cut the flattened and air-dried cork oak bark into boards with a length ⅹ width of 650 mm ⅹ 150 mm, and send it to a sander to set the thickness and sand it for later use;
[0033] Step 4: Arrange the cork oak bark that has been sanded to a certain thickness vertically on the plate frame, open the valve of the hot water pipe, and spray 100°C hot water on the cork oak bark board to keep the cork oak bark Plate flushing state for 1.5 hours;
[0034] Step 5: Afte...
Embodiment 2
[0051] A kind of concrete steps of the processing method of cork oak bark yoga column are:
[0052] Step 1: Pick and peel off the fresh bark of the evergreen tree Quercus cork, brush off the moss and impurities on the surface, unfold it while it is wet, stack 18 layers alternately, and press heavy objects on the layers;
[0053] Step 2: After the bark of the cork oak becomes flat under the pressure of heavy objects, spread it out in the open air for half a year to dry naturally, and reserve it;
[0054] Step 3: Cut the flattened and air-dried cork oak bark into boards with a length ⅹ width of 650 mm ⅹ 150 mm, and send it to a sander to set the thickness and sand it for later use;
[0055] Step 4: Arrange the cork oak bark that has been sanded to a certain thickness vertically on the plate frame, open the valve of the hot water pipe, and spray 100°C hot water on the cork oak bark board to keep the cork oak bark Plate flush state for 1.8 hours;
[0056] Step 5: After the cork ...
Embodiment 3
[0073] A kind of concrete steps of the processing method of cork oak bark yoga column are:
[0074] Step 1: Pick and peel off the fresh bark of the evergreen tree Quercus cork, brush off the moss and impurities on the surface, unfold it while it is wet, stack 20 layers of staggered stacks, and press heavy objects on the stacks;
[0075] Step 2: After the bark of the cork oak becomes flat under the pressure of heavy objects, spread it out in the open air for half a year to dry naturally, and reserve it;
[0076] Step 3: Cut the flattened and air-dried cork oak bark into boards with a length ⅹ width of 650 mm ⅹ 150 mm, and send it to a sander to set the thickness and sand it for later use;
[0077] Step 4: Arrange the cork oak bark that has been sanded to a certain thickness vertically on the plate frame, open the valve of the hot water pipe, and spray 100°C hot water on the cork oak bark board to keep the cork oak bark Plate flush state for 2 hours;
[0078] Step 5: After the...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com