[0014] In the present embodiment, the preparation method of anti-skid stationery pen cover comprises the following steps:
[0015] (1) By weight, the following raw materials are equipped: hydrogenated styrene-isoprene-styrene block copolymer 25%, paraffin oil 20%, homopolypropylene 10%, calcium carbonate 8%, ethylene- Acrylic copolymer 12%, hydrogenated styrene-butadiene-styrene block copolymer 11%, silicon-based thermoplastic vulcanizate 13.9%, antioxidant 0.1%;
[0016] (2) Add hydrogenated styrene-isoprene-styrene block copolymer and paraffin oil into a stirring container with a stirrer, and stir evenly (the rotating speed of the stirrer is 900 rpm, and the stirring time is 15 minutes ), and then stand at room temperature for 18 hours (usually at 20-30° C. for 18 hours), to obtain mixture A;
[0017] (3) Homopolypropylene, ethylene-acrylic acid copolymer, hydrogenated styrene-butadiene-styrene block copolymer, calcium carbonate, silicon-based thermoplastic vulcanizate and ...
Embodiment 2
[0023] In the present embodiment, the preparation method of anti-skid stationery pen cover comprises the following steps:
[0024] (1) By weight, the following raw materials are equipped: hydrogenated styrene-isoprene-styrene block copolymer 20%, paraffin oil 28%, homopolypropylene 15%, calcium carbonate 8%, ethylene- Acrylic copolymer 10%, hydrogenated styrene-butadiene-styrene block copolymer 8%, silicon-based thermoplastic vulcanizate 10.9%, antioxidant 0.1%;
[0025] (2) Add hydrogenated styrene-isoprene-styrene block copolymer and paraffin oil into a stirring container with a stirrer, and stir evenly (the rotating speed of the stirrer is 800 rpm, and the stirring time is 10 minutes ), and then stand at room temperature for 12 hours (usually at 20-30° C. for 12 hours), to obtain mixture A;
[0026] (3) Homopolypropylene, ethylene-acrylic acid copolymer, hydrogenated styrene-butadiene-styrene block copolymer, calcium carbonate, silicon-based thermoplastic vulcanizate and a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com