Method for treating circulating cooling water of high-speed trains
A technology for circulating cooling water and treatment methods, which is applied in water/sludge/sewage treatment, special treatment targets, chemical instruments and methods, etc., and can solve problems such as accelerated corrosion and prone to corrosion.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment approach
[0017] According to one embodiment, the total iron content of the high-iron circulating cooling water is 3.0-5.0 mg / L.
[0018] In this embodiment, the complexing agent is selected from one of the following combinations: disodium edetate, sodium alginate and hydroxylamine hydrochloride, triethanolamine, sodium citrate and tartaric acid, sodium citrate, Triethanolamine and Disodium EDTA, Potassium Sodium Tartrate, Sodium Gluconate and Sodium Alginate, Sodium Gluconate, Dimercaptopropanol and Triethanolamine, Sodium Alginate, Potassium Sodium Tartrate and Citric Acid, Hydroxylamine Hydrochloride, Dimercapto Propanol and potassium sodium tartrate, dimercaptopropanol, hydroxylamine hydrochloride and citrate, citric acid, tartaric acid and sodium gluconate, tartaric acid, citric acid and dimercaptopropanol.
[0019] Preferably, the complexing agent is selected from one of the following combinations: potassium sodium tartrate, sodium gluconate and sodium alginate, sodium alginate, p...
Embodiment 1-10 and comparative example 1-2
[0048] Add compound complexing agent (composed of complexing agent A, complexing agent B and complexing agent C) to test water 1 and test water 2 respectively, and scale and corrosion inhibitor 1 by 100 mg / L Concentrations were added to test water 1 and 2 respectively, so that the effective concentrations of PBTCA, HEDP, and terpolymer in water were 4mg / L, 4mg / L, and 8mg / L respectively. The types and dosages of the agents are listed in Table 2.
Embodiment 11
[0050] Process test water 1 and 2 according to the method of Example 1, the difference is that the scale and corrosion inhibitor 2 of the same quality is used to replace the scale and corrosion inhibitor 1 of Example 1, so that sodium hexametaphosphate, HPAA and binary The effective concentrations of the copolymers are 4mg / L, 4mg / L and 8mg / L respectively.
PUM
Property | Measurement | Unit |
---|---|---|
Corrosion rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com