Photocatalyst partner
A photocatalyst and partner technology, applied in the directions of alkali metal oxides/hydroxides, inorganic chemistry, gas treatment, etc., can solve problems such as health hazards, easy damage to furniture, etc., to improve the environment, convenient for spraying, and fast effect. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0019] The preparation of montmorillonite-loaded chitosan among the present invention can adopt following method to prepare, and 0.855g chitosan chitosan quaternary ammonium salt is added into 250mL distilled water, stirs in boiling water until dissolving; Cool down to 25~30 °C to obtain chitosan quaternary ammonium salt solution. Disperse 5.0 g of nano-montmorillonite in 250 mL of distilled water to obtain a 2% montmorillonite suspension. Slowly add the above-mentioned chitosan quaternary ammonium salt solution into the nano-montmorillonite suspension, and then stir at 50° C. for 10 days. Wash with distilled water, filter, and vacuum dry for later use.
[0020] The preparation method of the photocatalyst partner of the present invention is as follows: firstly add citric acid monohydrate into deionized water and stir for 10 minutes, then add tetraethoxysilane and stir for 10 minutes, then add penetrant JFC and stir for 10 minutes, then add organosilicon disinfectant The foami...
Embodiment 1
[0022] A kind of photocatalyst companion of the present embodiment, comprises the composition of following percentage by weight, monohydrate citric acid 1%; Titanium dioxide 1.8% of 5nm, nanometer montmorillonite loaded chitosan quaternary ammonium salt 1%, carbamate starch 1.2% , tetraethoxysilane 5%; penetrant JFC 0.1%; silicone defoamer 0.01%; phytic acid 0.02%; glycerin 2.0%, food flavor 0.2%, deionized water balance.
Embodiment 2
[0024] A kind of photocatalyst companion, comprises the composition of following percentage by weight, monohydrate citric acid 2%; Titanium dioxide 1% of 5nm, nanometer montmorillonite loaded chitosan quaternary ammonium salt 1.5%, carbamate starch 1.5%, tetraethoxylate 6% base silane; 0.3% penetrant JFC; 0.05% organic silicon defoamer; 0.01% phytic acid; 2.5% glycerin, 0.3% food flavor, deionized water balance.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com