A free radical and radioactive technology, applied in chemical instruments and methods, chemical/physical/physical chemical processes, chemical/physical processes, etc., can solve the problems of high energy consumption and poor maintenance-free, and achieve low energy consumption and no maintenance. , the effect of high efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] A specific embodiment of a filler capable of generating free radicals according to the present invention, the described filler capable of generating free radicals is composed of a photocatalyst and a radioactive ore, the shape of the radioactive ore is spherical particles, and the radioactive ore is radium stone.
[0035] The spherical particles of the radioactive ore have a diameter of 6mm.
[0036] Of course, in different embodiments, the above-mentioned diameters can be adjusted to some extent.
[0037] The radioactivity requirements of the radioactive ore are: the dose rate at a distance of 1 meter from 20 kg of radioactive ore particles is not higher than 2.5 μsV / h; the weight ratio of the photocatalyst to the radioactive ore particles is 3:2.
[0038] The filler capable of generating free radicals also includes a binder, the photocatalyst and the binder form an outer coating structure, and the photocatalyst and the binder are powders.
[0039] The photocatalyst ...
Embodiment 2
[0047] The principle of embodiment 2 is the same as that of embodiment 1, the difference is:
[0048] A filler capable of generating free radicals in the present invention is composed of a photocatalyst and radioactive ore, the shape of the radioactive ore is spherical particles, and the radioactive ore is thorite. The diameter of the spherical particles of the thorite is 2 mm.
[0049] The preparation method of the filler capable of generating free radicals of the present invention may further comprise the steps:
[0050] In step (2), 30 kg of spherical thorite particles with a diameter of 2 mm were weighed for use as a spare.
[0051] In step (3), add 3 times the weight of water to the above-mentioned outer coating part and stir evenly to form a slurry, and put it into a disc granulator together with the above-mentioned spherical radium stone particles for uniform contact.
Embodiment 3
[0053] The principle of embodiment 3 is the same as that of embodiment 1, the difference is:
[0054] A filler capable of generating free radicals of the present invention is composed of a photocatalyst and a radioactive ore, the shape of the radioactive ore is spherical particles, and the radioactive ore is radium stone. The diameter of the spherical particles of the radium stone is 10mm.
[0055] The preparation method of the filler capable of generating free radicals of the present invention may further comprise the steps:
[0056] In step (2), 30 kg of spherical radium stone particles with a diameter of 10 mm are weighed for use as a spare.
[0057]In step (3), add 2.5 times the weight of water to the outer coating part and stir evenly to form a slurry, and put it into a disc granulator together with the spherical radium stone particles for uniform contact.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com