A technology for the preparation of waste emulsion and pulverized coal, which is applied in the petroleum industry, solid fuel, fuel and other directions, can solve the problems of high treatment cost, poor treatment effect and complex treatment process of cold rolling waste emulsion slag, so as to realize the utilization of waste. , easy to operate, low cost of preparation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] The preparation method of composite pulverized coal with cold-rolled waste emulsion slag added in this embodiment includes the following steps: first put the cold-rolled waste emulsion slag and economizer sedimentation ash into a mixer in a weight ratio of 1:2.5 and stir well The mixed material is obtained; the mixed material and steam coal are put into a mixer in a weight ratio of 1:9 for stirring, and then put into a coal mill for pulverization to obtain composite coal powder.
[0026] The weight loss of the composite coal powder prepared by the above composite coal powder preparation method of adding waste emulsion slag from cold rolling, heating the composite coal powder at 850°C for 5min, 10min, 15min, 20min, 25min, 30min, 35min, and 40min As shown in Table 1.
Embodiment 2
[0028] The preparation method of composite pulverized coal with cold-rolled waste emulsion slag added in this embodiment includes the following steps: first put the cold-rolled waste emulsion slag and economizer sedimentation ash into a mixer in a weight ratio of 1:2.5 and stir well The mixture is obtained; the mixture and steam coal are put into a mixer in a weight ratio of 2:8 for stirring, and then put into a coal mill for pulverization to obtain composite pulverized coal.
[0029] The weight loss of the composite coal powder prepared by the above composite coal powder preparation method of adding waste emulsion slag from cold rolling, heating the composite coal powder at 850°C for 5min, 10min, 15min, 20min, 25min, 30min, 35min, and 40min As shown in Table 1.
PUM
Property | Measurement | Unit |
---|---|---|
heat | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com