Preparation method of environment-friendly and energy-saving material
A technology of environmental protection, energy saving and preparation steps, applied in the field of building materials, can solve the problems of easy cracking, inconvenience, insufficient stability in use, etc., and achieve the effects of long-lasting color, wide source of raw materials, and remarkable thermal insulation effect.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A preparation method of an environment-friendly and energy-saving material, comprising the following preparation steps:
[0024] a. Mix fly ash, natural zeolite powder, bamboo charcoal fiber, polyimide fiber and wood cellulose into a pulverizer, pulverize and stir evenly to obtain a base material;
[0025] b. Add modified acrylic emulsion, vegetable oil and pine nut extract to the base material, heat and stir at 90°C for 30 minutes, then add water reducer and mugwort leaf extract, and heat in a water bath at 60°C for 1 hour to obtain material 1;
[0026] c. Mix water-based monomer, polyethylene, butyl acrylate, methyl methacrylate and styrene-butadiene rubber in a mixer, and heat at 180°C until completely melted to obtain material 2;
[0027] d. Add a coupling agent and a stabilizer to material 2, and stir for 30 minutes at a speed of 300 r / min to obtain material 3;
[0028] e. Mix material 1 and material 3 evenly, heat and stir at 55°C to form a slurry, then add a sur...
Embodiment 2
[0037] A preparation method of an environment-friendly and energy-saving material, comprising the following preparation steps:
[0038] a. Mix fly ash, natural zeolite powder, bamboo charcoal fiber, polyimide fiber and wood cellulose into a pulverizer, pulverize and stir evenly to obtain a base material;
[0039] b. Add modified acrylic emulsion, vegetable oil and pine nut extract to the base material, heat and stir at 80°C for 30 minutes, then add water reducer and mugwort leaf extract, and heat in a water bath at 50°C for 1 hour to obtain material 1;
[0040] c. Mix water-based monomer, polyethylene, butyl acrylate, methyl methacrylate and styrene-butadiene rubber in a mixer, and heat at 160°C until completely melted to obtain material 2;
[0041] d. Add a coupling agent and a stabilizer to material 2, and stir for 30 minutes at a speed of 200r / min to obtain material 3;
[0042] e. Mix material 1 and material 3 evenly, heat and stir at 55°C to form a slurry, then add a surf...
Embodiment 3
[0051] A preparation method of an environment-friendly and energy-saving material, comprising the following preparation steps:
[0052] a. Mix fly ash, natural zeolite powder, bamboo charcoal fiber, polyimide fiber and wood cellulose into a pulverizer, pulverize and stir evenly to obtain a base material;
[0053] b. Add modified acrylic emulsion, vegetable oil and pine nut extract to the base material, heat and stir at 90°C for 40 minutes, then add water reducer and mugwort leaf extract, and heat in a water bath at 60°C for 2 hours to obtain material 1;
[0054] c. Mix water-based monomer, polyethylene, butyl acrylate, methyl methacrylate and styrene-butadiene rubber in a mixer, and heat at 180°C until completely melted to obtain material 2;
[0055] d. Add coupling agent and stabilizer to material 2, and stir for 35 minutes at a speed of 300r / min to obtain material 3;
[0056] e. Mix material 1 and material 3 evenly, heat and stir at 65°C to form a slurry, then add a surfact...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com