A production process and fiber fabric technology, which is applied in fiber treatment, phosphorus organic compounds, textiles and papermaking, etc., can solve the problems of large equipment occupation, long process route, high energy consumption, etc., achieve low CMC value and reduce environmental pollution , good biodegradability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] A process for preparing an unsymmetrical bisamide sulfonic acid phosphate salt, comprising the following steps:
[0018] 1. Add 1.0 mol ricinoleic acid and active agent potassium hydroxide (according to 1.5% of the mass of ricinoleic acid) into a reactor equipped with a condenser, thermometer and agitator, start stirring, and raise the temperature to 90°C under nitrogen protection , slowly add 1.1mol triethylenetetramine dropwise to the reactor, and drop it completely within 1 hour, then react at a constant temperature of 150-160°C for 6h, cool to room temperature, and obtain the intermediate monoamide, which is then added in the reactor Add 1mol dehydroabietic acid, start stirring, raise the temperature to 90°C under nitrogen protection, then react at a constant temperature of 150-160°C for 6h, cool to room temperature, use 150# solvent oil and butanone mixed solvent (volume ratio 1:1 ) recrystallized 3 times, removed by-products, and dried in a vacuum oven at 60°C to ...
Embodiment 2
[0022] A process for preparing an unsymmetrical bisamide sulfonic acid phosphate salt, comprising the following steps:
[0023] 1. Add 1.0 mol ricinoleic acid and active agent potassium hydroxide (according to 1.5% of the mass of ricinoleic acid) into a reactor equipped with a condenser, thermometer and agitator, start stirring, and raise the temperature to 90°C under nitrogen protection , slowly add 1.1mol triethylenetetramine dropwise to the reactor, and drop it completely within 1 hour, then react at a constant temperature of 150-160°C for 6h, cool to room temperature, and obtain the intermediate monoamide, which is then added in the reactor Add 1mol dehydroabietic acid, start stirring, raise the temperature to 90°C under nitrogen protection, then react at a constant temperature of 150-160°C for 6h, cool to room temperature, use 150# solvent oil and butanone mixed solvent (volume ratio 1:1 ) recrystallized 3 times, removed by-products, and dried in a vacuum oven at 60°C to ...
Embodiment 3
[0027] A process for preparing an unsymmetrical bisamide sulfonic acid phosphate ester salt, comprising the following steps:
[0028] 1. Add 1.0 mol ricinoleic acid and active agent potassium hydroxide (according to 1.5% of the mass of ricinoleic acid) into a reactor equipped with a condenser, thermometer and agitator, start stirring, and raise the temperature to 90°C under nitrogen protection , slowly add 1.3mol triethylenetetramine dropwise to the reactor, and the dropwise addition is completed within 1 hour, then react at a constant temperature of 150-160°C for 6h, and cool to room temperature to obtain an intermediate monoamide, which is then added in the reactor Add 1.1mol of dehydroabietic acid, start stirring, heat up to 90°C under nitrogen protection, then react at a constant temperature of 150-160°C for 6h, cool to room temperature, use 150# solvent oil and butanone mixed solvent (volume ratio 1: 1) Recrystallize 3 times, remove by-products, dry in a vacuum oven at 60...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com