Manufacturing technique for antibacterial anti-cracking plastic basin
A production process and plastic technology, applied in the field of plastic basin production, can solve the problems of acne on the face, breeding bacteria, bacterial infection of women, etc., and achieve the effects of convenient preparation, low price and broad market prospects.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] The invention relates to a production process of an antibacterial and anti-crack plastic pot. The raw materials of the anti-bacterial and anti-crack plastic pot are: 40-50 parts of phenolic resin, 22-28 parts of polyethylene, 15-25 parts of EPDM rubber powder, poly Olefin elastomer POE10-12 parts, antibacterial powder 4-6 parts, alum 10-12 parts.
[0012] The production process is as follows:
[0013] Step 1: Weigh 40 parts of phenolic resin, 22 parts of polyethylene, 15 parts of EPDM rubber powder, 10 parts of polyolefin elastomer POE, 4 parts of antibacterial powder, and 10 parts of alum;
[0014] Step 2: heating the raw material obtained in Step 1 to a high temperature until it melts into a liquid state, and the temperature is 130-150 degrees Celsius;
[0015] Step 3: The mixture obtained in Step 2 is automatically put into the injection mold through the assembly line, and formed through the procedures of filling, compression molding, pressure holding, cooling, warp...
Embodiment 2
[0019] The invention relates to a production process of an antibacterial and anti-crack plastic pot. The raw materials of the anti-bacterial and anti-crack plastic pot are: 40-50 parts of phenolic resin, 22-28 parts of polyethylene, 15-25 parts of EPDM rubber powder, poly Olefin elastomer POE10-12 parts, antibacterial powder 4-6 parts, alum 10-12 parts.
[0020] The production process is as follows:
[0021] Step 1: Weigh 50 parts of phenolic resin, 28 parts of polyethylene, 25 parts of EPDM rubber powder, 12 parts of polyolefin elastomer POE, 6 parts of antibacterial powder, and 12 parts of alum;
[0022] Step 2: heating the raw material obtained in Step 1 to a high temperature until it melts into a liquid state, and the temperature is 130-150 degrees Celsius;
[0023] Step 3: The mixture obtained in Step 2 is automatically put into the injection mold through the assembly line, and formed through the procedures of filling, compression molding, pressure holding, cooling, warp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com