Building internal wall coating and preparation method thereof
A technology for building interiors and coatings, applied in the field of interior wall coatings and coatings, can solve problems such as air pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Embodiment 1: a kind of building interior wall coating is made by the raw material of following weight ratio:
[0027] Architectural interior paint active ingredient 30g
[0028] Adsorbent diatomaceous earth 10g
[0029] Binder polyvinyl alcohol 10g
[0030] Dispersant hydroxymethylcellulose 5g
[0031] Stabilizer xanthan gum 5g
[0032] Film-forming emulsion styrene-acrylic emulsion 700g
[0033] water 240g
[0034] The preparation method of above-mentioned building interior wall paint, prepares according to the following method:
[0035] In the 2L reactor, the temperature of the water bath is controlled at 60 o C, add 700g film-forming emulsion styrene-acrylic emulsion, 240g water, 30g architectural interior wall paint active ingredient, 10g adsorbent 100 mesh diatomite, 10g binder polyvinyl alcohol, 5g dispersant hydroxymethyl cellulose and 5g The stabilizer xanthan gum is ground and stirred for 8 hours to obtain a uniformly mixed architectural interior wall p...
Embodiment 2
[0041] Embodiment 2: a kind of building interior wall paint, is made of the raw material of following weight ratio:
[0042] Architectural interior paint active ingredient 50g
[0043] Adsorbent diatomaceous earth 20g
[0044] Binder polyvinyl alcohol 20g
[0045] Dispersant Hydroxyethylcellulose 10g
[0046] Stabilizer xanthan gum 10g
[0047] Film-forming emulsion acrylic emulsion 800g
[0048] water 90g
[0049] The preparation method of above-mentioned building interior wall paint, prepares according to the following method:
[0050] In the 2L reactor, the temperature of the water bath is controlled at 80 o C, add 800g film-forming emulsion acrylic emulsion, 90g water, 50g building interior wall paint active ingredient, 20g adsorbent 200 mesh diatomite, 20g binder polyvinyl alcohol, 10g dispersant hydroxyethyl cellulose and 10g stabilizer Add xanthan gum, grind and stir for 12 hours to get a uniformly mixed architectural interior wall paint.
[0051] The preparatio...
Embodiment 3
[0056] Embodiment 3: a kind of building interior wall paint, is made of the raw material of following weight ratio:
[0057] Architectural interior paint active ingredient 40g
[0058] Adsorbent diatomaceous earth 15g
[0059] Binder polyvinyl alcohol 15g
[0060] Dispersant Hydroxypropyl Cellulose 8g
[0061] Stabilizer xanthan gum 7g
[0062] Film-forming emulsion silicone acrylic emulsion 750g
[0063]water 165g
[0064] The preparation method of above-mentioned building interior wall paint, prepares according to the following method:
[0065] In the 2L reactor, the temperature of the water bath is controlled at 70 o C, add 750g film-forming emulsion silicone acrylic emulsion, 165g water, 40g architectural interior wall paint active ingredient, 15g adsorbent 150 mesh diatomite, 15g binder polyvinyl alcohol, 8g dispersant hydroxypropyl cellulose and 7g The stabilizer xanthan gum is ground and stirred for 10 hours to obtain a uniformly mixed architectural interior wall...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com