Environment-friendly type high-performance bait brightener
A brightening agent and high-performance technology, applied in the direction of coating, etc., can solve the problem of unsatisfactory fishing effect, etc., and achieve the effect of good compatibility, environmental protection and bright color
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] An environment-friendly high-performance brightening agent for fishing lures, which is made of the following components in parts by weight: divalent ester 60, PVC powder 25, free radical photoinitiator 5, ethyl acetate 8, polyvinyl butyral 8. Liquid paraffin 2.5, magnetized water 7.
[0031] The preparation method is as follows:
[0032] (1) Get the PVC powder of feeding amount and add magnetized water and fully mix, make PVC powder wet, set aside;
[0033] (2) Take the amount of dibasic acid ester, heat it to 52-65°C, put in wet PVC powder, stir for 10 minutes, then put in liquid paraffin, stir evenly, and obtain feed liquid I;
[0034] (3) Add the free radical photoinitiator of the feeding amount into the feed liquid I, stir evenly, and obtain the feed liquid II;
[0035] (4) Add the polyvinyl butyral of the feeding amount into the feed liquid II, stir evenly, and obtain the feed liquid III;
[0036] (5) Add the amount of ethyl acetate into the feed liquid III, dis...
Embodiment 2
[0038] An environment-friendly high-performance brightening agent for fishing lures, which is made of the following components in parts by weight: divalent ester 65, PVC powder 30, free radical photoinitiator 8, ethyl acetate 15, polyvinyl butyral 10. Liquid paraffin 5. Magnetized water 10.
[0039] The preparation method is as follows:
[0040] (1) Get the PVC powder of feeding amount and add magnetized water and fully mix, make PVC powder wet, set aside;
[0041] (2) Take the amount of dibasic acid ester, heat it to 52-65°C, put in wet PVC powder, stir for 10 minutes, then put in liquid paraffin, stir evenly, and obtain feed liquid I;
[0042] (3) Add the free radical photoinitiator of the feeding amount into the feed liquid I, stir evenly, and obtain the feed liquid II;
[0043] (4) Add the polyvinyl butyral of the feeding amount into the feed liquid II, stir evenly, and obtain the feed liquid III;
[0044] (5) Add the amount of ethyl acetate into the feed liquid III, di...
Embodiment 3
[0046] An environment-friendly high-performance brightening agent for fishing lures, which is made of the following components in parts by weight: dibasic acid ester 70, PVC powder 15, free radical photoinitiator 3, ethyl acetate 5, polyvinyl butyral 5. Liquid paraffin 3. Magnetized water 5.
[0047] The preparation method is as follows:
[0048] (1) Get the PVC powder of feeding amount and add magnetized water and fully mix, make PVC powder wet, set aside;
[0049] (2) Take the amount of dibasic acid ester, heat it to 52-65°C, put in the wet PVC powder, stir for 10 minutes, then put in liquid paraffin, stir evenly, and obtain the feed liquid I;
[0050] (3) Add the free radical photoinitiator of the feeding amount into the feed liquid I, stir evenly, and obtain the feed liquid II;
[0051] (4) Add the polyvinyl butyral of the feeding amount into the feed liquid II, stir evenly, and obtain the feed liquid III;
[0052] (5) Add the amount of ethyl acetate into the feed liqui...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com