A polyacrylamide, heavy metal ion technology, applied in chemical instruments and methods, water/sludge/sewage treatment, water/sewage treatment, etc. Heavy metal ion wastewater treatment requirements and other issues, to achieve the effect of small impact on water quality, easy operation and good separation effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0048] The preparation method of the magnetic gelatin-based anionic polyacrylamide heavy metal ion remover of the present embodiment comprises:
[0049] (1) Preparation of gelatin-based anionic polyacrylamide: Add appropriate amount of deionized water into the reactor, add 0.4g gelatin, 2g acrylamide, stir evenly, then add 0.6g maleic anhydride, stir evenly, heat up to 50 -100°C. Weigh 0.1-2.0% potassium persulfate in the total amount of reaction monomers, dissolve it with an appropriate amount of water, slowly add potassium persulfate aqueous solution to the above reaction system dropwise within 10-30 minutes, and then react for 30-120 minutes. After the temperature drops to room temperature, adjust the pH value to 6-9 with an appropriate amount of sodium hydroxide aqueous solution;
[0050] (2) Preparation of magnetic gelatin-based anionic polyacrylamide: heat the above-mentioned gelatin-based anionic polyacrylamide aqueous solution to 50-100°C, add Fe with 10% mass of acry...
Embodiment 2
[0052] The preparation method of the magnetic gelatin-based anionic polyacrylamide heavy metal ion remover of the present embodiment comprises:
[0053] (1) Preparation of gelatin-based anionic polyacrylamide: Add appropriate amount of deionized water into the reactor, add 1g of gelatin and 2g of acrylamide, stir evenly, then add 2g of sodium vinyl sulfonate, stir evenly, weigh the reaction monomer The total amount of 0.1-2.0% sodium thiosulfate is dissolved with an appropriate amount of water and added to the reaction system, and the temperature is raised to 50-100°C. Weigh hydrogen peroxide with the same molar amount of sodium thiosulfate, slowly add hydrogen peroxide dropwise into the above reaction system within 10-30 minutes, and react for another 30-120 minutes. After the temperature drops to room temperature, adjust the pH value to 6-9 with an appropriate amount of sodium hydroxide aqueous solution;
[0054] (2) Preparation of magnetic gelatin-based anionic polyacrylam...
Embodiment 3
[0056] The preparation method of the magnetic gelatin-based anionic polyacrylamide heavy metal ion remover of the present embodiment comprises:
[0057] (1) Preparation of gelatin-based anionic polyacrylamide: Add appropriate amount of deionized water into the reactor, add 0.6g gelatin, 2g acrylamide, stir well, then add 1.2g 2-acrylamide-2-methylpropylphosphine Acid, stir evenly, weigh 0.1-2.0% sodium thiosulfate of the total amount of reaction monomers, dissolve it with an appropriate amount of water, add it to the reaction system, and raise the temperature to 50-100°C. Weigh ammonium persulfate with the same molar weight as sodium thiosulfate, and dissolve it with an appropriate amount of water. Slowly add the ammonium persulfate aqueous solution dropwise into the above reaction system within 10-30 minutes, and then react for 30-120 minutes. After the temperature drops to room temperature, adjust the pH value to 6-9 with an appropriate amount of sodium hydroxide aqueous so...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com