An industrial sewage and adsorbent technology, which is applied in water/sewage treatment, adsorbed water/sewage treatment, water/sludge/sewage treatment, etc., can solve the problems of complex regeneration, difficult to use on a large scale, and expensive activated carbon. Good formability, low cost and considerable economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] An adsorbent for industrial sewage treatment, its raw materials include by weight: 30 parts of attapulgite, 40 parts of clay, 20 parts of expanded graphite cyclodextrin compound, 18 parts of bamboo charcoal, 10 parts of carbon nanotubes, 10 parts of loofah, 8 parts of adhesive, 35 parts of flocculant, 3 parts of oxidative fungicide.
Embodiment 2
[0020] An industrial sewage treatment adsorbent, its raw materials include by weight: 40 parts of attapulgite, 30 parts of clay, 30 parts of expanded graphite cyclodextrin compound, 10 parts of bamboo charcoal, 20 parts of carbon nanotubes, 5 parts of loofah, 18 parts of binder, 20 parts of flocculant, 5 parts of oxidative fungicide.
[0021] The expanded graphite cyclodextrin compound is prepared by the following process: mix and stir expanded graphite and water, adjust the temperature, add sodium hydroxide, urea and rice husk fiber to stir, cool down, keep warm, heat up, add sulfuric acid solution to adjust the pH value of the system to a Neutral, filter, wash with water, dry, pulverize, then immerse in silica suspension and stir, spray dry, add β-cyclodextrin, sodium hydroxide, pyridine, mix and stir, add succinic anhydride, adjust temperature, stir, add Dimethylformamide yields expanded graphitic cyclodextrin complexes.
Embodiment 3
[0023] An adsorbent for industrial sewage treatment, its raw materials include by weight: 28 parts of attapulgite, 32 parts of pottery clay, 25 parts of expanded graphite cyclodextrin compound, 12 parts of bamboo charcoal, 18 parts of carbon nanotubes, 6 parts of loofah, 16 parts of sodium carboxymethyl cellulose, 24 parts of calcium polyacrylate, 4.6 parts of oxidative fungicide.
[0024] The expanded graphite cyclodextrin compound is prepared by the following process: 20 parts by weight of expanded graphite and 400 parts of water are mixed and stirred for 40 minutes, the stirring speed is 1000 r / min, the temperature is adjusted to 2 °C, 35 parts of sodium hydroxide, 4 parts of Stir urea and 60 parts of rice husk fiber for 55 minutes, cool down to -25°C, keep warm for 1 hour, heat up to 45°C, add sulfuric acid solution to adjust the pH value of the system to neutral, filter, wash with water, dry, crush, and then immerse at a concentration of 1wt % of the silica suspension was...
PUM
Property | Measurement | Unit |
---|---|---|
adsorption capacity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com