Enriched superphosphate and preparation method for same
A technology rich in calcium superphosphate and sulfuric acid, applied in fertilizer mixtures, fertilization devices, applications, etc., can solve the problems of high quality requirements and long curing time of phosphoric acid and phosphate rock powder, and achieve good social and economic benefits and wide sources of raw materials , the effect of broad market prospects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] The calcium superphosphate-enriched product is composed of 20-40 parts of carboapatite, 5-15 parts of sulfuric acid, 5-15 parts of spent acid and 5-15 parts of activated loosening agent according to weight.
[0035] Described calcium superphosphate rich and preparation method thereof comprise the following steps:
[0036] (1) Mixing sulfuric acid and waste acid to prepare mixed acid A;
[0037] (2) Mix and react the prepared mixed acid A with carbonapatite, heat and stir for 2-6 hours to obtain product B;
[0038] (3) The prepared product B is added with an activating loosening agent, stacked and matured for 12-16 days, granulated, dried, sieved, and cooled to obtain the product.
Embodiment 2
[0040] By weight, it consists of 30 parts of carboapatite, 10 parts of sulfuric acid, 10 parts of waste acid and 10 parts of activated loosening agent.
[0041] (1) Mixing sulfuric acid and waste acid to prepare mixed acid A;
[0042] (2) Mix and react the prepared mixed acid A with carbonapatite, heat and stir for 4 hours to obtain product B;
[0043] (3) The prepared product B is added with an activating loosening agent, stacked, matured and neutralized for 14 days, granulated, dried, sieved and cooled to obtain the product.
Embodiment 3
[0045] A superphosphate-rich calcium superphosphate is composed of 20 parts of carboapatite, 5 parts of sulfuric acid, 5 parts of spent acid and 5 parts of activated loosening agent by weight.
[0046] Described calcium superphosphate rich and preparation method thereof comprise the following steps:
[0047] (1) Mixing sulfuric acid and waste acid to prepare mixed acid A;
[0048] (2) Mix and react the prepared mixed acid A with carbonapatite, heat and stir for 2 hours to obtain product B;
[0049] (3) The prepared product B is added with an activating loosening agent, stacked, matured and neutralized for 12 days, granulated, dried, sieved and cooled to obtain the product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com