Embodiment 1
[0019] Embodiment 1: the preparation of a kind of pearlescent popping pearls for cigarettes, the specific steps are as follows:
[0020] (1) According to the following formula table, prepare the binder solution in the pearlescent coating film material for cigarettes:
[0021] Formula table of binder solution in pearlescent coating film material for cigarettes
[0022] Raw material type Specification weight ratio Adhesive Hydroxypropyl Cellulose 10 water pure water 90
[0023] Add all the weight parts of the adhesive in the above formula into water at 25±5°C, stir for 0.5 hours to dissolve into an aqueous solution of the adhesive, and let stand for defoaming for 2 hours;
[0024] (2) Place the shaped and dried pop-up beads for cigarettes in a CF granulation coating machine, and add the aqueous binder solution prepared in step (1) into the solution spraying device of the coating machine. The addition of the aqueous solution of the mixture accou...
Embodiment 2
[0027] Embodiment 2: the preparation of a kind of pearlescent popping pearls for cigarettes, the specific steps are as follows:
[0028] (1) According to the following formula table, prepare the binder solution in the pearlescent coating film material for cigarettes:
[0029] Formula table of binder solution in pearlescent coating film material for cigarettes
[0030] Raw material type Specification weight ratio Adhesive Hydroxypropyl cellulose: carboxymethyl cellulose is 2:1 20 water pure water 80
[0031] Add all the weight parts of the adhesive in the above formula into water at 25±5°C, stir for 1 hour to dissolve into an aqueous adhesive solution, and let it stand for defoaming for 5 hours;
[0032] (2) Place the shaped and dried pop-up beads for cigarettes in a CF granulation coating machine, and add the aqueous binder solution prepared in step (1) into the solution spraying device of the coating machine. The addition of the aqueous solu...
Embodiment 3
[0035] Embodiment 3: the preparation of a kind of pearlescent popping pearls for cigarettes, the specific steps are as follows:
[0036] (1) According to the following formula table, prepare the binder solution in the pearlescent coating film material for cigarettes:
[0037] Formula table of binder solution in pearlescent coating film material for cigarettes
[0038] Raw material type Specification weight ratio Adhesive Povidone: carboxymethyl cellulose is 1:1 35 water pure water 65
[0039] Add all the weight parts of the adhesive in the above formula into water at 25±5°C, stir for 2 hours to dissolve into an aqueous adhesive solution, and let it stand for 8 hours to defoam;
[0040] (2) Place the shaped and dried pop-up beads for cigarettes in a CF granulation coating machine, and add the aqueous binder solution prepared in step (1) into the solution spraying device of the coating machine. The addition of the mixture aqueous solution is 10...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com