Environment-friendly water-soluble anti-caking agent, and preparation method and application thereof
An anti-caking agent, water-soluble technology, applied in application, nitrogen fertilizer, inorganic fertilizer, etc., can solve the problems of water-soluble powder agglomeration, high use cost, easy caking, etc., and achieve the goal of enhancing resistance, improving quality and output Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0025] The preparation method of above-mentioned anti-caking agent, comprises the following steps:
[0026] 1) Mix aluminum potassium sulfate, aluminum ammonium sulfate and sodium lauryl sulfate according to the proportion to obtain a mixed powder, and mix and pulverize the mixed powder;
[0027] 2) Under the condition of a shearing force of 2300-2600r / min, the particles of the mixed powder are made uniform, and the particle size of the mixed powder after shearing is 800-1000 mesh.
[0028] The above-mentioned anti-caking agent can be applied in the coating process of water-soluble chemical fertilizers, and the steps of the coating process are as follows:
[0029] Put the water-soluble fertilizer and anti-caking agent into the coating machine, the addition of the anti-caking agent is 5-10‰ of the weight of the water-soluble fertilizer, and stir, the stirring speed is 40-60r / min, and the stirring time is 8 -12min, so that the water-soluble fertilizer and anti-caking agent are ...
Embodiment 1
[0031] An environment-friendly water-soluble anti-caking agent, which is prepared from the following components by weight percentage:
[0032]
[0033] Among them, the fineness of aluminum potassium sulfate is 600-700 mesh, the fineness of aluminum ammonium sulfate is 600-700 mesh, and the fineness of sodium lauryl sulfate is 600-700 mesh.
[0034] The preparation method of this anti-caking agent comprises the following steps:
[0035] 1) Mix aluminum potassium sulfate, aluminum ammonium sulfate and sodium lauryl sulfate according to the proportion to obtain a mixed powder, and mix and pulverize the mixed powder;
[0036] 2) Under the condition of a shearing force of 2300r / min, the particles of the mixed powder are uniform, and the particle size of the mixed powder after shearing is 800 mesh.
Embodiment 2
[0038] An environment-friendly water-soluble anti-caking agent, which is prepared from the following components by weight percentage:
[0039] Potassium Aluminum Sulfate 15%
[0040] Ammonium Aluminum Sulfate 12%
[0041] Sodium Lauryl Sulfate 73%;
[0042] Among them, the fineness of aluminum potassium sulfate is 600-700 mesh, the fineness of aluminum ammonium sulfate is 600-700 mesh, and the fineness of sodium lauryl sulfate is 600-700 mesh.
[0043] The preparation method of this anti-caking agent comprises the following steps:
[0044] 1) Mix aluminum potassium sulfate, aluminum ammonium sulfate and sodium lauryl sulfate according to the proportion to obtain a mixed powder, and mix and pulverize the mixed powder;
[0045] 2) Under the condition of a shearing force of 2400r / min, the particles of the mixed powder are uniform, and the particle size of the mixed powder after shearing is 1000 mesh.
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com