Embodiment 1
[0015] A low-cost waterproof and aging-resistant building brick proposed by the present invention, its raw materials include by weight: 0.5 parts of ethylene-vinyl acetate copolymer, 2.5 parts of hydroxypropyl methylcellulose, 0.4 parts of polysiloxane powder, modified 16 parts of natural montmorillonite, 10 parts of fly ash, 16 parts of calcium hydroxide, 20 parts of clay, 16 parts of stone waste, 3 parts of silicon nitride, 9 parts of diatomite, 3 parts of magnesium oxide, 35 parts of cement, clay 10 servings.
Embodiment 2
[0017] A low-cost waterproof and aging-resistant building brick proposed by the present invention, its raw materials include by weight: 1.5 parts of ethylene-vinyl acetate copolymer, 1.5 parts of hydroxypropyl methylcellulose, 0.8 parts of polysiloxane powder, modified 8 parts of natural montmorillonite, 20 parts of fly ash, 8 parts of calcium hydroxide, 30 parts of clay, 8 parts of stone waste, 7 parts of silicon nitride, 3 parts of diatomite, 7 parts of magnesium oxide, 25 parts of cement, clay 20 servings.
[0018] The modified montmorillonite is prepared by the following process: mix and stir montmorillonite powder, oxalic acid solution, and sodium dihydrogen phosphate solution, adjust the pH value of the system to 5.2-6.2, stir, let stand, extract the upper suspension, and suspend it to the upper layer Add sodium hydroxide to the system pH value to 11-11.8, stir, add oxalic acid solution until the system pH value reaches 9.5-10, stir, add potassium dihydrogen phosphate un...
Embodiment 3
[0020] A low-cost waterproof and aging-resistant building brick proposed by the present invention, its raw materials include by weight: 0.9 parts of ethylene-vinyl acetate copolymer, 2.2 parts of hydroxypropyl methylcellulose, 0.5 parts of polysiloxane powder, modified 14 parts of natural montmorillonite, 12 parts of fly ash, 14 parts of calcium hydroxide, 23 parts of clay, 14 parts of stone waste, 4 parts of silicon nitride, 7 parts of diatomite, 4 parts of magnesium oxide, 32 parts of cement, clay 14 servings.
[0021] The modified montmorillonite is prepared by the following process: 60 parts by weight of montmorillonite powder, 40 parts of oxalic acid solution with a concentration of 12 wt%, and 50 parts of sodium dihydrogen phosphate solution with a concentration of 5 wt% were mixed and stirred for 20 minutes, and the pH value of the system was adjusted. to 5.2-6.2, stirred for 180min, stood still for 8h, extracted the upper suspension, added sodium hydroxide to the upper...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com