A technology of nanocellulose and composite materials, which is applied in the field of electrochromic nanocellulose composite materials and its preparation, can solve the problems of less research on flexible electrochromic materials, and achieves simple preparation method, low environmental pollution and application prospect. huge effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] An electrochromic nanocellulose composite material, comprising nanocellulose, polyethylene glycol and aniline, the solvent is N, N-dimethylacetamide, wherein, by mass ratio, nanocellulose: polyethylene glycol: aniline =84:3:13; the concentration of nanocellulose in the solvent is 0.5g / ml; the relative molecular weight of polyethylene glycol is 6000;
[0024] A preparation method of electrochromic nano-cellulose composite material, comprising the following steps:
[0025] (1) According to the above ratio, in a three-necked flask, dissolve nanocellulose, polyethylene glycol, aniline, in N,N-dimethylacetamide, and heat to 70°C in a water bath for 4 hours to obtain Mixed solution of nanocellulose;
[0026] (2) The mixed solution of nanocellulose is placed on the film-forming mold, and evaporated at 60°C under vacuum conditions to obtain a nanocellulose film; the thickness of the film is 10nm;
[0027] (3) in N 2 Under protection, place the nanocellulose film on the tray ...
Embodiment 2
[0030] An electrochromic nanocellulose composite material, comprising nanocellulose, polyethylene glycol and aniline, the solvent is N, N-dimethylacetamide, wherein, by mass ratio, nanocellulose: polyethylene glycol: aniline =87:3:10; the concentration of nanocellulose in the solvent is 1.0g / ml; the relative molecular weight of polyethylene glycol is 4000;
[0031] A preparation method of electrochromic nano-cellulose composite material, comprising the following steps:
[0032] (1) According to the above ratio, in a three-necked flask, dissolve nanocellulose, polyethylene glycol, aniline, in N,N-dimethylacetamide, and heat to 80°C in a water bath for 1 hour to obtain Mixed solution of nanocellulose;
[0033] (2) The mixed solution of nanocellulose is placed on a film-forming mold, and evaporated at 70°C under vacuum conditions to obtain a nanocellulose film; the film thickness is 50nm;
[0034] (3) Under the protection of Ar gas, place the nanocellulose film on the tray of t...
Embodiment 3
[0037] An electrochromic nanocellulose composite material, comprising nanocellulose, polyethylene glycol and aniline, the solvent is N, N-dimethylacetamide, wherein, by mass ratio, nanocellulose: polyethylene glycol: aniline =87:3:10; the concentration of nanocellulose in the solvent is 1.0g / ml; the relative molecular weight of polyethylene glycol is 4000;
[0038] A preparation method of electrochromic nano-cellulose composite material, comprising the following steps:
[0039] (1) According to the above ratio, in a three-necked flask, dissolve nanocellulose, polyethylene glycol, aniline, in N,N-dimethylacetamide, and heat to 80°C in a water bath for 1 hour to obtain Mixed solution of nanocellulose;
[0040] (2) The mixed solution of nanocellulose is placed on a film-forming mold, and evaporated at 70°C under vacuum conditions to obtain a nanocellulose film; the film thickness is 50nm;
[0041] (3) Under the protection of Ar gas, place the nanocellulose film on the tray of t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology