Coating process of plasterboard exterior laminated layer
A coating process and gypsum board technology, which is applied to the device, coating, special surface and other directions of coating liquid on the surface, can solve the problems of high cost, many processes, long construction period, etc., to improve the coating quality and reduce the cost. , The effect of simplifying the coating process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] 1. Attach a layer of kraft cardboard-like gypsum board on the surface to connect the gap, and use the method of scraping putty to make the surface of the joint smooth, and the height of the putty surface at the joint is less than 0.5mm above the surface of the gypsum board. And the joints and plasterboard surface are excessively smooth.
[0018] 2. Set the temperature of the coating environment at about 6°C and the relative humidity at about 40%; use water-based latex paint as the coating material, and adjust the viscosity of the water-based latex paint to 4000mpa.s; choose 200-250mm rolling short-haired wool brush.
[0019] 3. Start painting, the method of painting is roller brush and roller coating, the coating speed is controlled at 0.5m / s, the coating thickness is 30μm / time, and the roller coating is 3 times with an interval of 2 hours between each time. The total thickness is controlled at 90 μm.
[0020] 4. After the coating is completed, the inspection is carri...
Embodiment 2
[0022] 1. A layer of glass fiber cloth is attached to the outer surface of the gypsum board, and the gap between the gypsum boards is connected, and the putty method is used to make the surface of the joint smooth, and the putty surface at the joint is higher than the height of the surface of the gypsum board Less than 0.5mm, and the joints and the surface of the gypsum board are too smooth.
[0023] 2. Set the temperature of the coating environment at about 10°C and the relative humidity at about 50%; use water-based latex paint as the coating material, and adjust the viscosity of the water-based latex paint to 5000mpa.s; use a spray gun for spraying.
[0024] 3. Start coating, the coating method is spraying method, the coating speed is controlled at 0.6m / s, the coating thickness is 40μm / time, spraying 3 times, each interval is 3 hours, the total thickness of coating is 120 μm.
[0025] 4. After the coating is completed, the visual inspection method is used. The appearance o...
PUM
Property | Measurement | Unit |
---|---|---|
viscosity | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com