[0020] In the first step, graphene, acetylene black, and PVB are weighed according to the weight ratio of (85):(10):(5), and dispersed in NMP at 30°C for 1 hour before use;
[0021] In the second step, the uniformly dispersed slurry in the first step is evenly coated on a copper strip with a width of 1000 mm and a thickness of 0.3 mm to form a graphene coating, and then dried at 90 ° C to obtain a graphene-coated surface. Copper strip;
[0022] In the third step, the side of the copper strip attached with graphene is folded in half from the middle, and folded into the same size so as to be re-stacked for the next cycle. The copper strip is annealed at 330°C for 1 hour;
[0023] In the fourth step, the rolled graphene copper strip is processed according to the second and third steps. This process is repeated 7 times to accumulate enough strain, and the grains are refined. At the same time, the graphene is evenly distributed on the copper strip. For the inner nano-graphene cop...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com