Embodiment 1
[0032] Such as figure 1 As shown, the anti-mosquito and washable fabric includes a fabric 1 , a mosquito-proof layer 2 attached to the base of the fabric 1 , and a wash-resistant layer 3 attached to the mosquito-proof layer 2 .
[0033] Pyrethroid insecticides 4 and carbamate insecticides 5 are dispersed in the anti-mosquito layer 1 , and carbamate insecticides 5 are dispersed in the water-resistant layer 3 .
[0034] The fabric 1 is a mosquito net cloth with full polyester hexagonal mesh, the specifications are: 100D, 36filaments, 40g / m 2 , white; the pyrethroid insecticide 4 is cis-cypermethrin, and the carbamate insecticide 5 is difencarb.
[0035] The preparation method of the above-mentioned anti-mosquito washable fabric is as follows:
[0036] The first finishing process:
[0037] Preparation of anti-mosquito finishing liquid: first weigh appropriate amount of cis-cypermethrin, dicarbacarb, acrylic adhesive and water-based polyurethane curing agent and place them in f...
Embodiment 2
[0052] The fabric 1 is pure cotton and white.
[0053] The pyrethroid insecticide 4 is cyfluthrin, and the carbamate insecticide 5 is propoxur.
[0054] The preparation method of the above-mentioned anti-mosquito washable fabric is as follows:
[0055] The first finishing process:
[0056] Preparation of anti-mosquito finishing solution: first weigh appropriate amount of cyfluthrin, propoxur, acrylic adhesive and water-based polyurethane curing agent and place them in four glass beakers respectively, then add appropriate amount of deionized water into the beakers, and then use Stir with a glass rod so that the reagent and water can dissolve well. Finally, mix the four reagents diluted with deionized water and stir evenly with a glass rod. The concentration of cyfluthrin in the mosquito repellent finishing solution is 4g / L. The concentration of Granville is 50g / L, the concentration of acrylic adhesive is 70g / L, and the concentration of water-based polyurethane curing agent is...
Embodiment 3
[0063] The fabric 1 is nylon and white.
[0064] The pyrethroid insecticide 4 is phenothrin, and the carbamate insecticide 5 is carnavir.
[0065] The preparation method of the above-mentioned anti-mosquito washable fabric is as follows:
[0066] The first finishing process:
[0067] Preparation of anti-mosquito finishing liquid: first weigh appropriate amount of phenothrin, carnavir, acrylic adhesive and water-based polyurethane curing agent and place them in four glass beakers respectively, then add appropriate amount of deionized water into the beakers , and then stirred with a glass rod, so that the reagent and water can be well miscible, finally mixed the four reagents diluted with deionized water, and stirred evenly with a glass rod, the concentration of phenothrin in the mosquito repellent finishing solution is 5g / L, the concentration of carbavir is 30g / L, the concentration of acrylic adhesive is 90g / L, and the concentration of water-based polyurethane curing agent is...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com