Preparing method for cigarette tipping paper resisting hemodia
A tooth sensitivity, tipping paper technology, applied in tobacco, cigar manufacturing, defoaming agent, etc., to achieve the effect of reducing tooth sensitivity, reducing tooth root inflammation, and repairing oral mucosa
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] (1) Weigh the following raw materials in parts by weight: 1 part of strontium oxide, 1 part of potassium chloride, 2 parts of hydroxyapatite, 1 part of sodium monofluorophosphate, 2 parts of Chinese herbal medicine extract, 3 parts of talcum powder, 6 parts of vinyl butyral, 0.3 part of vegetable oil, 1 part of defoamer, 20 parts of ethanol, uniformly mixed to obtain the first mixture;
[0018] (2) Add pure water to the first mixture obtained in step (1), 30 parts by weight, and stir to obtain the second mixture;
[0019] (3) adding the water-soluble acrylic resin that is 35 parts by weight in the second mixture that obtains in step (2) obtains anti-tooth hypersensitivity cigarette tipping paper coating;
[0020] (4) Apply the anti-tooth hypersensitivity cigarette tipping paper coating obtained in step (3) evenly on the surface of the tobacco tipping paper, dry and gilt to obtain the anti-tooth hypersensitivity cigarette tipping paper.
Embodiment 2
[0022] (1) Weigh the following raw materials in parts by weight: 1 part of strontium oxide, 1 part of potassium chloride, 3 parts of hydroxyapatite, 2 parts of sodium monofluorophosphate, 3 parts of Chinese herbal medicine extract, 3 parts of talcum powder, 6 parts of vinyl butyral, 0.3 part of vegetable oil, 1 part of defoamer, 20 parts of ethanol, uniformly mixed to obtain the first mixture;
[0023] (2) Add pure water to the first mixture obtained in step (1), 35 parts by weight, and stir to obtain the second mixture;
[0024] (3) adding the water-soluble acrylic resin that is 35 parts by weight in the second mixture that obtains in step (2) obtains anti-tooth hypersensitivity cigarette tipping paper coating;
[0025] (4) Apply the anti-tooth hypersensitivity cigarette tipping paper coating obtained in step (3) evenly on the surface of the tobacco tipping paper, dry and gilt to obtain the anti-tooth hypersensitivity cigarette tipping paper.
Embodiment 3
[0027] (1) Weigh the following raw materials in parts by weight: 1 part of strontium oxide, 2 parts of potassium chloride, 3 parts of hydroxyapatite, 2 parts of sodium monofluorophosphate, 5 parts of Chinese herbal medicine extract, 3 parts of talcum powder, 6 parts of vinyl butyral, 0.3 part of vegetable oil, 1 part of defoamer, 20 parts of ethanol, uniformly mixed to obtain the first mixture;
[0028] (2) Add pure water to the first mixture obtained in step (1), 40 parts by weight, and stir to obtain the second mixture;
[0029] (3) adding the water-soluble acrylic resin that is 35 parts by weight in the second mixture that obtains in step (2) obtains anti-tooth hypersensitivity cigarette tipping paper coating;
[0030] (4) Apply the anti-tooth hypersensitivity cigarette tipping paper coating obtained in step (3) evenly on the surface of the tobacco tipping paper, dry and gilt to obtain the anti-tooth hypersensitivity cigarette tipping paper.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com