A kind of preparation method of tensile cotton and its products
A technology of tension cotton and silkworm cocoons, which is applied in the field of silk cotton, can solve the problems of airtightness, poor elasticity, and dampness of warm clothes, and achieve the effects of improving elasticity and high tensile strength, reducing elongation loss at break, and reducing loss of breaking strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0055] The preparation method of a kind of stretch cotton provided by embodiment 1 of the present invention comprises the following steps:
[0056] (1) Prepare the following raw materials: cocoon, spandex, elastin, distilled water, natural water, puffing agent, malic acid, silicone antibacterial agent, scouring agent;
[0057] (2) Carry out vacuum infiltration treatment on silkworm cocoons:
[0058] (2.1) The natural water is treated by using the salt-free regenerative hydrogen ion exchange method to obtain the treated aqueous solution, and the aqueous solution is heated to 52°C warm water;
[0059] (2.2) Treat silkworm cocoons with vacuum infiltration equipment outside the machine and inhale warm water, move the treated silkworm cocoons to the cocoon storage box, and then move the silkworm cocoons to the low-temperature penetration section, cooking chamber, adjustment section, and outlet protection section of the cocoon cooking machine in sequence With the outlet section, os...
Embodiment 2
[0086] The main difference between this embodiment and Embodiment 1 is that it also includes the following steps: (8) Carry out health care treatment on the stretch cotton after refining treatment:
[0087] (8.1) Prepare the following raw materials: 2.5% antibacterial finishing agent, 3.2% negative ion far-infrared finishing agent, 4.2% moisture-absorbing and breathable finishing agent;
[0088] (8.2) Mix 2.5% antibacterial finishing agent, 3.2% negative ion far-infrared finishing agent and 4.2% moisture-absorbing and breathable finishing agent to prepare a mixed finishing agent;
[0089] (8.2) Soak the tensile cotton in the mixed finishing agent for 10 minutes, dehydrate it, and dry it at 60°C.
[0090] Other steps are the same as those in Embodiment 1, and will not be repeated here.
Embodiment 3
[0092] The main difference between this example and Example 2 is that the following steps are carried out after the antibacterial treatment in the step (5): immerse the cocoon fiber in natural water for 15 minutes, and dry it so that the moisture content of the cocoon fiber is 32%. Seal it and place it in a liquid nitrogen tank to freeze for 70 hours, then take out the cocoon fiber and place it in a vacuum drying oven for rewarming.
[0093] Other steps are the same as those in Embodiment 2, and will not be repeated here.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com