Plantation wood modification processing method
A treatment method and technology for plantation, which are applied in the field of modification and treatment of plantation wood, can solve the problems of limiting the use effect and application field of plantation trees, poor plantation wood properties, poor dimensional stability, etc., and improve the application effect and application field. , The effect of improving permeability and improving surface hardness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A method for modifying plantation wood, comprising the following steps:
[0017] (1) Pretreatment: After peeling and sawing the selected fir into the required size specifications, dry it at 50°C-80°C for 8-24 hours, and control the moisture content of the wood to no higher than 25%. , and then microwave treatment for 10 to 30 minutes;
[0018] (2) Modifier equipment: add 100 parts by mass of water, 25 parts by mass of nano-calcium carbonate, 15 parts by mass of nano-silicon dioxide, and then add 1 part by mass of fatty alcohol polyoxyethylene ether into the mixer, and shake the mixture under ultrasonic vibration and Under high-speed stirring with a rotation speed not lower than 6000r / min, treat for 20 to 50 minutes, then add 15 parts by mass of zinc borate, 8 parts by mass of ammonium molybdate, 12 parts by mass of chlorothalonil, 10 parts by mass of sodium octaborate tetrahydrate, bis-octyl 5 parts by mass of base dimethyl ammonium chloride, and stir together evenly t...
Embodiment 2
[0022] A method for modifying plantation wood, comprising the following steps:
[0023] (1) Pretreatment: After the selected poplar is peeled and sawed into the required size specifications, it is dried at 50°C-80°C for 8-24 hours, and the moisture content of the wood is controlled not to be higher than 25. %, then microwave treatment for 10-30 minutes;
[0024] (2) Modifier equipment: Add 75 parts by mass of water, 20 parts by mass of nano-calcium carbonate, 10 parts by mass of nano-silicon dioxide, and then add 0.3 parts by mass of surfactant to the mixer. Under high-speed stirring at 6000r / min, process for 20-50min, then add 10 parts by mass of zinc borate, 2 parts by mass of ammonium molybdate, 8 parts by mass of chlorothalonil, 5 parts by mass of sodium octaborate tetrahydrate, dioctyldimethyl 2 parts by mass of ammonium chloride, and stir together evenly to obtain a composite wood modifier, wherein the nano-calcium carbonate is light calcium carbonate nanoparticles with...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com