A fireproof coating and lost foam technology, applied in the field of coatings, can solve problems such as complex construction, reduced transparency, and aesthetic impact, and achieve the effects of excellent acid and alkali corrosion resistance, stable chemical properties of coatings, and extended service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] A transparent fireproof coating for lost foam, characterized in that, each component of the raw material is prepared according to the following parts by weight:
[0015] 30 parts of methyl etherified amino resin, 20 parts of pentaerythritol triacrylate, 8 parts of sodium amino acid phosphate resin, 20 parts of melamine, 15 parts of ammonium polyphosphate, 2 parts of inorganic sodium phosphate, magnesium hydroxide and aluminum oxide in a molar ratio of 2:1 The composition consists of 1 part of smoke suppressant, 10 parts of titanium dioxide, 5 parts of tricresyl sulfate, and 7 parts of dispersant composed of simethicone oil and glyceryl stearate at a weight ratio of 1:1.
Embodiment 2
[0017] A transparent fireproof coating for lost foam, characterized in that, each component of the raw material is prepared according to the following parts by weight:
[0018] 35 parts of methyl etherified amino resin, 25 parts of pentaerythritol triacrylate, 10 parts of sodium amino acid phosphate resin, 25 parts of melamine, 18 parts of ammonium polyphosphate, 3 parts of inorganic sodium phosphate, magnesium hydroxide and aluminum oxide in a molar ratio of 2:1 The composition consists of 2 parts of smoke suppressant, 15 parts of titanium dioxide, 6 parts of tricresyl sulfate, and 8 parts of dispersant composed of simethicone oil and glyceryl stearate at a weight ratio of 1:1.
Embodiment 3
[0020] A transparent fireproof coating for lost foam, characterized in that, each component of the raw material is prepared according to the following parts by weight:
[0021] 40 parts of methyl etherified amino resin, 30 parts of pentaerythritol triacrylate, 12 parts of sodium amino acid phosphate resin, 30 parts of melamine, 20 parts of ammonium polyphosphate, 4 parts of inorganic sodium phosphate, magnesium hydroxide and aluminum oxide in a molar ratio of 2:1 The composition consists of 3 parts of smoke inhibitor, 20 parts of titanium dioxide, 7 parts of tricresyl sulfate, and 9 parts of dispersant composed of simethicone oil and glyceryl stearate in a weight ratio of 1:1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com