Environment-friendly pesticide adjuvant
An environmentally friendly pesticide and adjuvant technology, applied in the field of pesticides, can solve the problems of poor surface wettability and adhesion of fruit trees, poor pesticide efficacy and safety, and pesticides cannot meet the requirements of insecticidal sterilization, etc. Protection, residue reduction, long-lasting effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] An environment-friendly pesticide adjuvant, in parts by weight, comprises the following components:
[0025] 10 parts of talcum powder, 5 parts of sodium dodecylbenzenesulfonate,
[0026] 5 parts of alkylphenol polyoxyethylene ether, 3 parts of dispersant,
[0027] 2 parts of wetting agent, 4 parts of spreading agent,
[0028] 2 parts of nano-zinc oxide, 1 part of nano-titanium oxide.
[0029] Its preparation method comprises the following steps:
[0030] (1) Dissolve 5 parts of sodium dodecylbenzenesulfonate and 3 parts of dispersant in water, stir to dissolve the solid, and obtain a mixed solution;
[0031] (2) Add 10 parts of talcum powder and 2 parts of wetting agent to the mixed solution obtained in step (1), and ultrasonically disperse the talcum powder for 2 hours in the mixed solution;
[0032] (3) Add 5 parts of alkylphenol polyoxyethylene ether and 4 parts of spreading agent, heat the mixed solution to 50°C, and ultrasonicate for 30 minutes;
[0033] (4) ...
Embodiment 2
[0035] An environment-friendly pesticide adjuvant, in parts by weight, comprises the following components:
[0036] 15 parts of talcum powder, 8 parts of sodium dodecylbenzenesulfonate,
[0037] 10 parts of alkylphenol polyoxyethylene ether, 6 parts of dispersant,
[0038] 5 parts of wetting agent, 5 parts of spreading agent,
[0039] 3 parts of nano-zinc oxide, 3 parts of nano-titanium oxide.
[0040] Its preparation method comprises the following steps:
[0041] (1) Dissolve 8 parts of sodium dodecylbenzenesulfonate and 6 parts of dispersant in water, stir to dissolve the solid, and obtain a mixed solution;
[0042] (2) Add 15 parts of talcum powder and 5 parts of wetting agent to the mixed solution obtained in step (1), and ultrasonically disperse the talcum powder for 5 hours in the mixed solution;
[0043] (3) Add 10 parts of alkylphenol polyoxyethylene ether and 5 parts of spreading agent, heat the mixed solution to 50°C, and ultrasonicate for 60 minutes;
[0044] (...
Embodiment 3
[0046] An environment-friendly pesticide adjuvant, in parts by weight, comprises the following components:
[0047] 11 parts of talcum powder, 6 parts of sodium dodecylbenzenesulfonate,
[0048] 6 parts of alkylphenol polyoxyethylene ether, 4 parts of dispersant,
[0049] 3 parts of wetting agent, 4 parts of spreading agent,
[0050] 2 parts of nano-zinc oxide, 2 parts of nano-titanium oxide.
[0051] Its preparation method comprises the following steps:
[0052] (1) Dissolve 6 parts of sodium dodecylbenzenesulfonate and 4 parts of dispersant in water, stir to dissolve the solid, and obtain a mixed solution;
[0053] (2) Add 11 parts of talcum powder and 3 parts of wetting agent to the mixed solution obtained in step (1), and ultrasonically disperse the talcum powder for 3 hours in the mixed solution;
[0054] (3) Add 6 parts of alkylphenol polyoxyethylene ether and 4 parts of spreading agent, heat the mixed solution to 50°C, and sonicate for 40 minutes;
[0055] (4) Cool...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com