Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

A kind of oil penetrating polishing treatment agent for synthetic leather and preparation method thereof

A synthetic leather and treatment agent technology, which is applied in fiber treatment, textiles and papermaking, etc., can solve the problems of high manufacturing cost of treatment reagents, failure to satisfy consumers' demand for synthetic leather, and poor comprehensive treatment effect, and achieve clear color and hand feeling Unique, translucent effect on the leather surface

Active Publication Date: 2016-04-20
浙江宝泽高分子材料有限公司
View PDF6 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, the treatment effect of the existing oil-penetrating polishing treatment agent for synthetic leather can no longer meet consumers' requirements for the luster and transparency of synthetic leather. At the same time, the manufacturing cost of the treatment reagent is relatively high, and the comprehensive treatment effect is not good.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] The oil polishing treatment agent for synthetic leather is composed of the following components: 5 parts by weight of alkyd resin, 7 parts by weight of nitrocellulose, 20 parts by weight of cyclohexanone, 29 parts by weight of butyl ether, 17 parts by weight of ethyl ester, 2 parts by weight of silicon oxide matting powder, 1 part by weight of oleic acid amide, 1 part by weight of erucamide, 0.3 part by weight of cellulose acetate, 0.2 part by weight of antibacterial and antifungal agent, 1 part by weight of methylphenyl silicone oil, and 1 part by weight of dispersant share.

[0022] The preparation method of the above-mentioned synthetic leather oil polishing treatment agent is: under normal temperature and pressure, 2.5 parts by weight of alkyd resin, 3.5 parts by weight of nitrocellulose, 20 parts by weight of cyclohexanone, and 29 parts by weight of butyl ether , 17 parts by weight of ethyl ester, 2 parts by weight of silica matting powder, and 1 part by weight of ...

Embodiment 2

[0025] The oil polishing treatment agent for synthetic leather is composed of the following components: 9 parts by weight of alkyd resin, 11 parts by weight of nitrocellulose, 24 parts by weight of cyclohexanone, 33 parts by weight of butyl ether, 21 parts by weight of ethyl ester, two 6 parts by weight of silicon oxide matting powder, 4 parts by weight of oleic acid amide, 3 parts by weight of erucamide, 2 parts by weight of cellulose acetate, 1 part by weight of antibacterial and antifungal agent, 3 parts by weight of methylphenyl silicone oil, 4 parts by weight of dispersant share.

[0026] The preparation method of the above-mentioned synthetic leather oil polishing treatment agent is: under normal temperature and pressure, 4.5 parts by weight of alkyd resin, 5.5 parts by weight of nitrocellulose, 24 parts by weight of cyclohexanone, and 33 parts by weight of butyl ether , 21 parts by weight of ethyl ester, 6 parts by weight of silica matting powder, and 4 parts by weight ...

Embodiment 3

[0029] The oil polishing treatment agent for synthetic leather is composed of the following components: 7 parts by weight of alkyd resin, 9 parts by weight of nitrocellulose, 22 parts by weight of cyclohexanone, 31 parts by weight of butyl ether, 19 parts by weight of ethyl ester, 4 parts by weight of silica matting powder, 2 parts by weight of oleic acid amide, 1 part by weight of erucamide, 0.5 part by weight of cellulose acetate, 0.5 part by weight of antibacterial and antifungal agent, 1 part by weight of methylphenyl silicone oil, and 2 parts by weight of dispersant share.

[0030] The preparation method of the above-mentioned synthetic leather oil polishing treatment agent is: under normal temperature and pressure, 3.5 parts by weight of alkyd resin, 4.5 parts by weight of nitrocellulose, 22 parts by weight of cyclohexanone, and 31 parts by weight of butyl ether , 19 parts by weight of ethyl ester, 4 parts by weight of silica matting powder, and 2 parts by weight of disp...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to an oil-permeation polishing treatment agent for synthetic leather and a preparation method of the polishing treatment agent. The treatment agent is prepared from the following components: alkyd resin, nitrocotton, cyclohexanone, butyl ether, ethyl ester, silicon dioxide extinction powder, oleamide, erucyl amide, cellulose acetate, an antibacterial and anti-mildew agent, methyl phenyl silicone oil and a dispersing agent. The oil-permeation polishing treatment agent is a novel material for later printing of the synthetic leather; the treatment agent can enable the synthetic leather to have remarkable temperature tolerance, to be embossed, have excellent glossy and oil waxy effects after being polished, and have special hand feeling, and the leather surface treated by the treatment agent is glossy and natural, and has clear color, excellent permeation feeling, strong leather effect and good general effect.

Description

technical field [0001] The present invention relates to the field of oil polishing treatment agent for synthetic leather, in particular, relates to an oil polishing treatment agent for synthetic leather used in the back-stage process of synthetic leather, and the present invention also relates to the oil polishing treatment agent for synthetic leather Preparation. Background technique [0002] Synthetic leather has the advantages of convenient processing, uniform quality, and various varieties, and has a wide range of applications. Surface treatment technology can process synthetic leather into different surface styles to meet people's requirements for various styles of synthetic leather surfaces. However, with the advancement of production technology, consumers have higher and higher requirements for the color, texture and feel of the leather surface. Not only must the color of the synthetic leather surface be guaranteed, but the transparency of the synthetic leather must ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): D06M15/51D06M15/07D06M15/643D06M11/79D06M13/41
Inventor 陈勇刚
Owner 浙江宝泽高分子材料有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products