A technology of concentrate and flotation, applied in flotation, solid separation, etc., can solve problems such as unstable heat balance in boiling roasting system, ineffective use of iron resources, complex composition of pulp in sulfur separation process, etc., to achieve great practicality and Economic benefits, adhere to energy saving and consumption reduction, and realize the effect of efficient utilization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Such as figure 1 As shown, after taking the ratio of Beijiang, Zhengyuan and Xinyuan mines (9:5:2), the sulfur and iron contents in the ore are 18.66% and 20.67% respectively.
[0037] The chemical composition of sulfur-containing gold concentrate 1 is as follows:
[0038] Table 1. Content of element 1 in sulfur-bearing gold concentrates (%)
[0039] element S(%) Fe(%) Cu(%) Zn(%) Pb(%) content 18.66 20.67 0.23 0.038 0.010 element As(%) Au (g / t) Ag (g / t) al 2 o 3 (%) SiO 2 (%) content 1.98 45.35 13.38 6.72 35.11
[0040] (1) rough selection
[0041]The gold concentrate with a sulfur content of 18.66% is mixed with water to form a 30%-35% slurry into the roughing tank, and sulfuric acid is added to stir for 3 minutes to keep the pH of the slurry at 5; add copper sulfate in sequence to each ton of gold concentrate 300-500 grams, stirred for 2 minutes; 320 grams of mercapto sulfide mineral collectors, stirred...
Embodiment 2
[0057] After taking Zaozigou, Tianhao, Beijiang, Zhengyuan, Xinyuan and Kunhe mines (45:18:18:10:4:18) as the ratio, the sulfur and iron contents in the ore are 14.06% and 14.63% respectively
[0058] The chemical composition of sulfur-containing gold concentrate 2 is as follows:
[0059] Table 3. Element 2 content of sulfur-bearing gold concentrate (%)
[0060] element S(%) Fe(%) Cu(%) Zn(%) Pb(%) content 14.06 14.63 0.19 0.047 0.015 element As(%) Au (g / t) Ag (g / t) al 2 o 3 (%) SiO 2 (%) content 2.74 44.30 9.52 8.64 38.15
[0061] (1) rough selection
[0062] The gold concentrate with a sulfur content of 14.06% is mixed with water to form a 30%-35% pulp into the roughing tank, and sulfuric acid is added to stir for 3 minutes to keep the pH of the pulp at 5; add copper sulfate in sequence to each ton of gold concentrate 300-500 grams, stirred for 2 minutes; 320 grams of mercapto sulfide mineral collectors, stirred...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com